MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Biomax® TPS 2700  (discontinued **)
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP

Material Notes: DuPont™ Biomax® TPS Injection molding resins can help reduce your footprint on the environment: they are a renewably soured and biodegradable solution delivering proven performance in molded articles. Traditional plastics used in packaging deliver high performance in most applications, but use depletable petroleum resources as their primary feedstock. DuPont™ Biomax® TPS Injection Molding resins can provide quality molded articles made from environmentally-friendly starch. The technology used for this unique material comes fro Plantic® Technologies, Ltd.
    Environmental value proposition:
  • Renewably sourced material solution
  • Biodegradable when in contact with water
  • Certified compostable in industrial composting conditions
  • Water flushable
    Performance attributes:
  • Good flexibility
  • Inherently grease-and oil-resistant
  • Sealable, printable, and laser etchable
  • Strong flavor and odor barrier
    Offering application versatility:
  • General purpose for most applications
  • High-flow for thing-wall applications
  • High-stiffness for more durable applications
  • 2 water-resistant grades: Limited contact with water is possible with the water-resistant grades; otherwise, for all other grades, water contact should be avoided.
DuPont™ Biomax® TPS is a renewably sourced offering that can be used in a variety of applications. It is especially appropriate for molded parts that will be used in mostly dry conditions prior to disposal. It offers disposal alternatives to landfills as it can biodegrade in natural environmental conditions. Biomax® TPS is a unique high-amylose starch material so it performs well as a stand-alone material option. Biomax® TPS starch feedstock is of non-genetically-modified origin. DuPont™ Biomax® TPS IM resins contain 53-93% renewaly sourced content by weight.
    Uses:
  • General Purpose
  • Packaging
  • Thin-walled Packaging

Processing Method: Injection Molding

    Availability:
  • Africa & Middle East
  • Asia Pacific
  • Europe
  • Latin America
  • North America
  • South America
Information provided by DuPont™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccASTM D1505
Melt Flow 4.7 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 52ASTM D2240
Tensile Strength at Break 7.50 MPaASTM D638
Elongation at Break 2.0 %ASTM D638
Tensile Modulus 0.630 GPaASTM D638
Izod Impact, Notched 31.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 44.9 °CUnannealed; ASTM D648
Vicat Softening Point 70.2 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 1.0 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Biomax® TPS 2501
DuPont Biomax® TPS 2100
Teknor Apex Terraloy™ BP 10000A Thermoplastic Starch + LLDPE
Celanese FORTRON 6165A4 PPS, 65% Mineral / Glass Reinforced
Teknor Apex Terraloy™ BP 20001A Thermoplastic Starch + Copolyester

PDUP971b / 133233

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.