MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group QSil 550 QSI Quantum Silicones Silicone Potting Material
Categories: Polymer; Thermoset; Silicone

Material Notes: QSil 550 is a 100% silicone solids elastomer designed for electrical potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairable.

Key Features:

  • 100% solids
  • Long gel time
  • Good elongation
  • Low modulus
Part of the Amber Chemical Group. Data provided by manufacturer.

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/cc"B" component
 1.41 g/cc"A" component
Viscosity 4000 cP"B" component
 4000 cP"A" component
Storage Temperature <= 38.0 °C12 months
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55cured 7 mins @ 150°C
Tensile Strength 3.52 MPacured 7 mins @ 150°C
Elongation at Break 150 %cured 7 mins @ 150°C
Tear Strength 33.0 plicured 7 mins @ 150°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.47e+15 ohm-cm
Dielectric Constant 3.1
@Frequency 1000 Hz
Dissipation Factor 0.0030
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.370 W/m-K
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -55.0 °C
Flammability, UL94 V-0
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Gel Time 130 min
 
Descriptive Properties
ColorBeige"A" component
 Black"B" component

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group QSil 551 QSI Quantum Silicones Silicone Potting Material
CHT Group QSil 430 QSI Quantum Silicones Silicone Potting Material
International Mold Steel TOOLOX® 44 Plastic and Rubber Mold Steel
CHT Group QSil 550R QSI Quantum Silicones Silicone Potting Material
CHT Group QSil 553 QSI Quantum Silicones Silicone Potting Material

PACC030 / 22157

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.