MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akro-Plastic Akromid® A3 GF 40 1 L black (4671) PA 6.6+PP Dry, 40% Glass Filled, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled; Nylon 66, Heat Stabilized; Polypropylene (PP)

Material Notes: Description: AKROMID A3 GF 40 1 L black (4671) is a 40% glass fiber reinforced, heat stabilized polyamide-blend with a reduced density compared to standard PA66 GF 40. Applications are mainly technical components in the automotive and electronic industry, where a weight and cost reduction is required.

Additive: Heat Stabilizer

Features:

  • High Stiffness
  • High Strength
  • Heat Stabilized
Uses:
  • Automotive Applications
  • Engineering Parts

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183
Filler Content 40 %ISO 1172
Moisture Absorption <= 1.0 %
@Temperature 70.0 °C
Humidity, 62% RH; ISO 1110
Linear Mold Shrinkage, Flow 0.0050 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cmISO 294-4
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
Spiral Flow 91.0 cmCross section: 7 mm x 3.5 mm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 170 MPa5 [mm/min]; ISO 527-2
Elongation at Break 2.9 %5 [mm/min]; ISO 527-2
Tensile Modulus 11800 MPa1 [mm/min]; ISO 527-2
Charpy Impact Unnotched 73.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 80.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 17.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 17.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °CDIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 260 °CUnannealed; ISO 75/B
Deflection Temperature at 1.8 MPa (264 psi) 246 °CUnannealed; ISO 75/A
Flammability, UL94 HB
@Thickness 0.800 mm
Glow Wire Ignition Temperature 775 °C
@Thickness 0.800 mm
IEC 60695-2-13
Glow Wire Flammability Index 750 °C
@Thickness 1.60 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 60.0 - 80.0 °C
Nozzle Temperature 270 - 290 °C
Zone 1 230 - 295 °C
Zone 2 230 - 295 °C
Zone 3 230 - 295 °C
Zone 4 230 - 295 °C
Melt Temperature 270 - 295 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Dry Time <= 2.00 hour
Hold Pressure 30.0 - 80.0 MPa
Back Pressure 5.00 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 40% Glass Fiber Filled
A. Schulman ComAlloy Comtuf® 103 Polypropylene, Glass Reinforced, Chemically Coupled, Impact Modified
Aclo Accutech Polypropylene Copolymer CP0436C10L Calcium Reinforced
Multibase Multi-Pro® 4003 R Medium Impact 40% Glass Filled Polypropylene
Overview of materials for Polypropylene with 30% Glass Fiber Filler

PAKRO211 / 182798

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.