MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo Technyl® C50H2 Nylon 6, Flame Retardant, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Information provided by Rhodia; Rhodia has been acquired by Solvay.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183-A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 80.0 MPa11600 psiISO 527
Tensile Modulus 3.70 GPa537 ksiISO 527
Flexural Strength 110 MPa16000 psiISO 178
Flexural Modulus 3.50 GPa508 ksiISO 178
Izod Impact, Notched 0.587 J/cm1.10 ft-lb/inISO 180
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index >= 600 V>= 600 V
Hot Wire Ignition, HWI  7.0 - 15 sec
@Thickness >=0.380 mm
7.0 - 15 sec
@Thickness >=0.0150 in
NC, BK, Gy colors
 7.0 - 15 sec
@Thickness >=0.750 mm
7.0 - 15 sec
@Thickness >=0.0295 in
All colors
 15 - 30 sec
@Thickness >=1.50 mm
15 - 30 sec
@Thickness >=0.0591 in
All colors
 30 - 60 sec
@Thickness >=3.00 mm
30 - 60 sec
@Thickness >=0.118 in
All colors
High Amp Arc Ignition, HAI  >= 120 arcs
@Thickness 0.380 mm
>= 120 arcs
@Thickness 0.0150 in
NC, BK, Gy colors
 >= 120 arcs
@Thickness 0.750 mm
>= 120 arcs
@Thickness 0.0295 in
All colors
 >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
All colors
 >= 120 arcs
@Thickness 3.00 mm
>= 120 arcs
@Thickness 0.118 in
All colors
High Voltage Arc-Tracking Rate, HVTR 0.000 - 254 mm/min0.000 - 10.0 in/min
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FISO 3146-C
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FISO 75-2
Flammability, UL94  V-0
@Thickness >=0.380 mm
V-0
@Thickness >=0.0150 in
NC, BK, Gy colors
 V-0
@Thickness >=0.750 mm
V-0
@Thickness >=0.0295 in
All colors
 V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
All colors
 V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
All colors

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® C 50 H2 PA6, DRY
Radici Radiflam® SFR (dry) Nylon 6
Celanese Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6
Domo Technyl® B 50H1 Nylon 66/6, Flame Retardant, EH0
Domo TechnylStar™ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant

PRHO25 / 123359

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.