MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ 5101-15 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: CALIBRE™ 5101 Polycarbonate resin is 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding UL94 flammability ratings and contains mold release. CALIBRE 5101 is available in 8 and 15 melt flow rates. CALIBRE 5101 resin has undergone biocompatibility testing based on ISO 10993 (Biological Evaluation of Medical Devices) and is suitable for use in approved medical applications.

Main Characteristics:

  • Glass reinforced
  • Ignition resistant
  • Tested under ISO 10993
Applications:
  • Information Technology Equipment
  • Telecommunications
  • Medical applications
Automotive Specifications:
  • FORD WSS-M4D309-C
  • GM.GMP.PC017

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccISO 1183/B
Water Absorption 0.15 %
@Time 86400 sec
ISO 62
Moisture Absorption at Equilibrium 0.25 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 in/inISO 294-4
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 62ASTM D785
Hardness, Rockwell R 122ASTM D785
Tensile Strength at Break 60.7 MPa50 mm/min; ASTM D638
 61.0 MPaISO 527-2/50
Tensile Strength, Yield 62.0 MPaISO 527-2/50
 62.1 MPa50 mm/min; ASTM D638
Elongation at Break 6.0 %50 mm/min; ASTM D638
 6.0 %ISO 527-2/50
Tensile Modulus 3380 MPa50 mm/min; ASTM D638
 3380 MPaISO 527-2/50
Flexural Strength 93.8 MPaMethod I (3 point load), 2.0 mm/min; ASTM D790
 94.0 MPa2.0 mm/min; ISO 178
Flexural Modulus 3170 MPaMethod I (3 point load), 2.0 mm/min; ASTM D790
 3170 MPa2.0 mm/min; ISO 178
Izod Impact, Notched 40.1 J/mASTM D3763
Tensile Impact Strength 147 kJ/m²ASTM D1822
Dart Drop, Total Energy 40.1 J3.39 m/sec; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 38.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 144 °CAnnealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 134 °CUnannealed; ISO 75-2/A
Vicat Softening Point 160 °CISO 306/B50
Flammability, UL94 V-2
@Thickness 1.60 mm
 V-0
@Thickness 3.20 mm
Oxygen Index 32 %ISO 4589-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 5101-8 Polycarbonate Resin
Trinseo CALIBRE™ 5201-8 Polycarbonate Resin
Trinseo CALIBRE™ 5201-12 Polycarbonate Resin
Trinseo CALIBRE™ 2061-15 Polycarbonate Resin
Trinseo EMERGE™ 8702 Polycarbonate

PDWST032 / 142241

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.