MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Proto Labs Inconel 718 - DMLS
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Proto Labs’ Inconel material is used in a DMLS process. Inconel is a high strength, corrosion resistant nickel chromium superalloy used at temperatures of -423F to 1300F. Its high-temperature strength is derived from its ability to create a thick, stable passivating oxide layer at high temperatures, protecting the material from further attack. Inconel also has good tensile, fatigue, creep and rupture strength. It is available in both high and normal resolution from Proto Labs.

Information provided by Proto Labs.

Key Words: Direct Metal Laser Sintering; EN DIN 1706:2013; 3D Printing; Additive Manufacturing
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 35.5
Tensile Strength, Ultimate 180 ksi
Tensile Strength, Yield 150 ksi
@Strain 0.2 %
Elongation at Break 6.0 - 12 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1300 °F
Minimum Service Temperature, Air -423 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCONEL® Alloy 718
MetalTek MTEK 718 Cast UNS N07718 Severe Corrosion and Heat Resistant Alloy
Universal Wire Works Inconel 718 (AMS 5832) Filler Metal
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed + Aged
Special Metals INCOLOY® alloy 908

NPROTO992 / 232386

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.