MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Saint-Gobain Tygon® PT-3350 Sanitary Silicone Tubing Formulation
Categories: Polymer; Thermoset; Silicone

Material Notes: Tygon® 3350: Designed for high-purity applications, Tygon® Sanitary Silicone Tubing's ultra-smooth inner bore can reduce the risk of particle entrapment and microscopic buildup during sensitive fluid transfer. In-house analysis of the inner surface of Tygon® Sanitary Silicone Tubing compared to other silicone tubing shows that it is up to three times smoother. Additionally, this smoother fluid path facilitates complete system cleaning and sterilization. Utilizing a platinum-curing process, Tygon® Sanitary Silicone Tubing eliminates the concern of extraction often encountered when alternative curing methods are used. It has also been fully characterized using the ISO 10993 standards, reducing user cost and time associated with process validation.

Features/Benefits:
  • Ultra-smooth inner bore reduces potential for particle entrapment
  • Minimal extractables help maintain fluid integrity
  • Documented biocompatibility for sensitive applications
  • Excellent fluid flow characteristics
  • Fully tested to ISO 10993 standards to facilitate validation process
Typical applications include Pharmaceutical and Cosmetic Processing, Medical Devices, Cell Harvest and Media Process Systems, Sterile Fill Lines, Water for Injection (WFI) Transfer, Chemistry and Blood Analyzers, Liquid Chromatography.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccASTM D792-91
Water Absorption 0.11 %24 hours at 23°C; ASTM D570-81
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 5015 seconds; ASTM D2240-91
Tensile Strength, Yield 1450 psiASTM D412-92
Elongation at Break 770 %ASTM D412-92
200% Modulus 0.280 ksi
@Strain 200 %
ASTM D412-92
Tear Strength 200 pliInitial Tear Strength; ASTM D624-91 Die B
Compression Set 7.0 %
@Temperature 70.0 °C
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
 35 %
@Temperature 175 °C
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 480 V/milASTM D149-93
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Brittleness Temperature -112 °FASTM D746-79
 
Descriptive Properties
ColorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex ELEXAR® EL 8421 Thermoplastic Elastomer
AlphaGary Evoprene™ LF 6150 Automotive Thermoplastic Elastomer
Aearo E-A-R Specialty Composites VersaDamp™ V-2550 TPE
Aearo E-A-R Specialty Composites VersaDamp™ V-2525 TPE
ExxonMobil Santoprene® 121-87 Thermoplastic Elastomer

PSTGQZ195 / 68709

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.