MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos Styrenics Avantra® 8550 Polystyrene (Discontinued)  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Flame Retardant

Material Notes: Ignition resistant grade of high impact polystyrene. It is free of polybrominated diphenylethers and meets UL94V-0 (@ 0.062"/1.6 mm min.) / 5VA (@ 0.125"/3.2 mm) ratings. It gives exceptional moldability while maintaining good mechanical and heat resistance properties.

Information provided by BASF.


Ineos Styrenics purchased this product line from BASF in 2005.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/cc
Moisture Absorption at Equilibrium <= 0.10 %
Water Absorption at Saturation <= 0.15 %
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cmASTM D955
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 200 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 23.0 MPa
Tensile Strength, Yield 23.0 MPa
Elongation at Break 30 %
Tensile Modulus 1.65 GPa
Flexural Modulus 1.93 GPa
Izod Impact, Notched 1.07 J/cmASTM D256A
Gardner Impact 6.00 J
@Thickness 3.17 mm
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C
Vicat Softening Point 98.0 °C
Flammability, UL94 V-0
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 240 °CMolding Temp

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 4140 Steel, normalized at 870°C (1600°F), air cooled, 13 mm (0.5 in.) round
Ineos Nova 4300 High Impact Polystyrene
Ineos Styrenics Polystyrene 476M (NAFTA)
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA)
Ineos Styrenics 495F High-Impact Polystyrene Resin (Global)

PSG004 / 67214

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.