MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schott NEO 1730 Alkaline Earth Aluminosilicate Glass
Categories: Ceramic; Glass

Material Notes: Alkaline earth aluminosilicate glass for high temperature applications in electrical engineering, for sealing to molybdenum, free from alkali

Bulb and exhaust tube for halogen lamps for automotive, household, and general lighting

The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppm

Information provided by SCHOTT AG.

Vendors: SCHOTT with its Business Unit Tubing offers tailor-made products & services worldwide from more than sixty special glass types for international growth markets such as industrial and environmental technology, electronics, display industry, architecture and design as well as pharmaceuticals. Contact us.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.67 g/cc
@Temperature 25.0 °C
 
Chemical PropertiesOriginal ValueComments
Acid Class, SR 1DIN 12116
Alkali Class, AR 2ISO 695
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.50 µm/m-°C
@Temperature 20.0 - 300 °C
ISO 7991
Transformation Temperature, Tg 715 °CISO 7884-8
Softening Point 935 °CViscosity 107.6 dPa s; ISO 7884-3
Working Point 1210 °CViscosity 104 dPa s; ISO 7884-2
Annealing Point 725 °CViscosity 1013 dPa s; ISO 7884-4
Strain Point 675 °CViscosity 1014.5 dPa s; ISO 7884-7
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.548
@Wavelength 587.6 nm
Transmission, Visible 37 %
@Thickness 1.00 mm,
Wavelength 585 nm
 65 %
@Thickness 1.00 mm,
Wavelength 750 nm
 88 %
@Thickness 1.00 mm,
Wavelength 775 nm
 87 - 90 %
@Wavelength 375 - 500 nm,
Thickness 1.00 mm
 88 - 90 %
@Wavelength 620 - 725 nm,
Thickness 1.00 mm
IR Transmittance 65 %
@Thickness 1.00 mm,
Wavelength 800 nm
UV Transmittance 12 %
@Thickness 1.00 mm,
Wavelength 300 nm
 58 %
@Thickness 1.00 mm,
Wavelength 330 nm
 72 %
@Thickness 1.00 mm,
Wavelength 340 nm
 
Component Elements PropertiesOriginal ValueComments
Alkalis <= 0.030 %Total Alkali Oxide
 
Descriptive Properties
Hydrolytic ResistanceClass HGB 1ISO 719

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott Glass 8240 Alkaline Earth Aluminosilicate Glass
Corning 1724 Aluminosilicate Crushed/Powdered Glass
Esstech V-115-1104 Aluminosilicate Glass-Ceramic
Schott Glass 8241 Alkaline Earth Aluminosilicate Glass
Schott Glass 8253 Alkaline Earth Aluminosilicate Glass

CSGS911 / 162016

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.