System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Durethan® A 30 000000 Nylon 6 (PA6), Dry
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Unreinforced
Material Notes:
PA 66, standard injection molding grade, non-reinforced, very easy release, normal solidification
Application Examples: terminal blocks, cable clips, bobbins, gearwheels
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.14
g/cc
ISO 1183
Moisture Absorption at Equilibrium
2.8 %
50% RH; ISO 62
Water Absorption at Saturation
8.5 %
IOS 62
Linear Mold Shrinkage, Flow
0.0118
cm/cm
150x105x3; ISO 2577
Linear Mold Shrinkage, Transverse
0.0195
cm/cm
150x105x3; ISO 2577
Mechanical Properties
Original Value
Comments
Ball Indentation Hardness
130
MPa
ISO 2093-1
Tensile Strength, Yield
85.0
MPa
50 mm/min; ISO 527-1,-2
Elongation at Yield
4.5 %
50 mm/min; ISO 527-1,-2
Tensile Modulus
3200
MPa
1 mm/min; ISO 527-1,-2
Flexural Strength
125
MPa
2 mm/min; ISO 178-A
Flexural Yield Strength
100
MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus
2800
MPa
2 mm/min; ISO 178-A
Flexural Strain at Break
6.0 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
<=
10.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1A
<=
10.0
kJ/m²
@Temperature -30.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO)
NB
@Temperature 23.0 °C
ISO 180-1U
NB
@Temperature -30.0 °C
ISO 180-1U
Charpy Impact Unnotched
NB
@Temperature 23.0 °C
ISO 180-1U
NB
@Temperature -30.0 °C
ISO 180-1U
Charpy Impact, Notched
<=
10.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1A
<=
10.0
kJ/m²
@Temperature -30.0 °C
ISO 180-1A
<=
10.0
kJ/m²
@Temperature -40.0 °C
ISO 180-1A
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+13
ohm-cm
IEC 60093
Surface Resistance
1.00e+15
ohm
IEC 60093
Dielectric Constant
3.4
@Frequency 1e+6 Hz
IEC 60250
3.8
@Frequency 100 Hz
IEC 60250
Dielectric Strength
30.0
kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor
0.0090
@Frequency 100 Hz
IEC 60250
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
550
V
Solution B; IEC 60112
600
V
Solution A; IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
90.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow
100
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point
263
°C
10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi)
70.0
°C
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
225
°C
ISO 75-1,-2
Deflection Temperature at 8.0 MPa
50.0
°C
ISO 75-1,-2
Vicat Softening Point
>=
230
°C
@Load 5.10 kg
120°C/h; ISO 306
>=
230
°C
@Load 5.10 kg
50°C/h; ISO 306
Flammability, UL94
V-2
@Thickness 0.750 mm
Oxygen Index
27 %
Method A; ISO 4589-2
Glow Wire Flammability Index
750
°C
@Thickness 2.00 mm
IEC 60695-2-12
Shrinkage, MD
0.26 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Shrinkage Flow Direction 150x105x3; ISO 2577
Shrinkage, TD
0.36 %
@Treatment Temp. 120 °C,
Time 14400 sec
150x105x3; ISO 2577
Processing Properties
Original Value
Comments
Melt Temperature
280
°C
Mold Temperature
80.0
°C
Back Pressure
50.0
MPa
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
LATI Latamid 6 H2 G/30-V2HF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Asahi Kasei Leona™ 91G60 Polyamide 66, MF Reinforced
Addiplast Addinyl PMD 20164 Nylon 6
Polynt HUP 45/27 LS RB-Colour
Plenco 6582 Phenolic, Briquette, Injection Molded
PLANW9558 / 207989
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.