MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PSC 1540(AS) Crystal Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Transparent Grade

Material Notes: 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact polystyrene. Having high gloss, it is particularly suitable for glossy-layer co-extrusion. In injection molding, 1541 possesses low viscosity at high shear rate. It combines excellent fluidity with a higher softening point. 1540 is not externally lubricated.

Application

Dairy sheet, Cups, Coextrusion crystal. 1541 Extrusion: Boxes, Petri dishes, medical products, Office equipment - e.g. filing trays, Pen bodies and toys, Internal fridge parts.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines. This product was previously known as LACQRENE®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccASTM D1505
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
Melt Flow 12 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238G
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 420 kg(f)/cm²ASTM D638M
Elongation at Break 2.0 %ASTM D638M
Flexural Yield Strength 75.0 kg(f)/cm²ASTM D790
Flexural Modulus 29000 kg(f)/cm²ASTM D790
Izod Impact, Notched 2.20 kg-cm/cmNotched/Unnotched not specified; ASTM D256A
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+14 ohmISO IEC93
Dielectric Strength 135 kV/mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 71.0 µm/m-°C
@Temperature 20.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °CASTM D648
Vicat Softening Point 86.0 °C50N (T° increase = 5°C/h); ASTM D1525B
 91.0 °C10N (T° increase = 50°C/h); ASTM D1525A
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 240 °C
Drying Temperature 70.0 °CPre drying temperature
Dry Time 2 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PSC 585 Polystyrene
Total PSC 1540(EU) Crystal Polystyrene
Total PSC 1960N Crystal Polystyrene
Total PSC 1340 Crystal Polystyrene
Total PSC 536 Polystyrene

PFINAA027 / 38463

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.