MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vycom CELTEC MARINE™ Expanded Foam PVC Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: Celtec Marine is made from rigid expanded foam polyvinyl chloride (PVC) material whose combination of features makes it ideal for wood trim and plywood replacement in boat manufacturing. Its closed cell structure does not absorb water and acts as a water barrier. Because of its staple pull and screw pull strength, Celtec Marine is ideal for applications in marine upholstery, seat backs, seat bottoms, trim for rough fiberglass openings, brackets, cabinets, draws etc.

FEATURES AND BENEFITS

  • Light weight- Celtec marine combines lightweight with strength to reduce weight in boat construction.
  • Strength- Celtec Marine has a high strength to weight ratio that makes it ideal for many boat building applications.
  • Superior workability- Celtec marine is easy to form, cut, glue, screw, nail, and staple.
  • Flammability- Celtec Marine meets UL guidelines, is self extinguishing and has a flame spread of 20.
  • Thermal conductivity- Celtec Marine is an excellent insulator.
  • Weatherability and water resistance- Celtec Marine is durable and will not absorb water.
  • Density- Celtec Marine is lighter than water and it floats.
  • Safety- Celtec Marine is Lead, cadmium, barium and zinc free.
  • Stability- Celtec Marine will not rot and it is cleanable and retains its color.
  • Economical- Celtec Marine is designed to last and it is economical to use.

Information provided by Compression Polymers Corp - Vycom

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.550 g/ccASTM D792
Water Absorption 0.15 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 2256 psiASTM D638
Tensile Modulus 144000 psiASTM D638
Flexural Strength 3329 psiASTM D790
Flexural Modulus 144200 psiASTM D790
Charpy Impact, Unnotched 4.50 ft-lb[ft-lb/in]; ASTM D256
Gardner Impact 8.60 ft-lbASTM D4228
 
Thermal PropertiesOriginal ValueComments
CTE, linear 32.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 150 °FASTM D648
Flame Spread Index 20ASTM E84
 
Descriptive Properties
Burning RateNo burn when flame removed
Nail Hold, Lbf/in penetration35ASTM D1761
Screw Hold, Lbf/in penetration680ASTM D1761
Staple Hold, Lbf/in penetration180ASTM D1761

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Axiall 3801 Vinyl Foam, Extrusion
Axiall 3803 Vinyl Foam, Extrusion
CoreLite PVC 48 Closed-Cell PVC Foam Sheet
Overview of materials for PVC, Foam Grade
Axiall 3802 Vinyl Foam, Extrusion

PCPCV14 / 29086

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.