MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kennametal Stellite Deloro® 55 Nickel Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: This gas-atomized powder is highly spherical particles with very low gas content. The alloy exhibits hard chromium borides and carbides in a nickel rich matrix. The alloy has excellent resistance to abrasion and good deposition characteristics.

Information provided by Kennametal Stellite™

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 52 - 57
 
Component Elements PropertiesOriginal ValueComments
Boron, B 2.7 %
Carbon, C 0.60 %
Chromium, Cr 12 %
Iron, Fe 4.0 %
Nickel, Ni >= 76.7 %as balance
Silicon, Si 4.0 %
 
Descriptive Properties
Application TechniqueHVOF & thermal spray
 PTA & laser deposition
 Spray-fuse & powder welding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kennametal Stellite Deloro® 60 Nickel Alloy
Kennametal Stellite Deloro® 50 Nickel Alloy
Kennametal Stellite Nucalloy® 488V High-Silicon Nickel-Base Hardfacing Alloy
Kennametal Stellite Deloro® 30 Nickel Alloy
Johnson Matthey Nickelbraze™ HTN3 Nickel Based Brazing Filler Metal

NSTA4950 / 159882

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.