MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ 201-10 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: CALIBRE™ 200-10 is produced in compliance with the US FDA and EU food contact regulations. It provides excellent impact resistance, heat distortion resistance and optical clarity. CALIBRE 200-10 product is formulated with mold release.

Applications:

  • Food processor housings
  • Liquid containers
  • Food utensils
  • Packaging applications
Govt. and Industry Standards:
  • US FDA 21 CFR 177.1580
  • Underwriters Laboratory (UL)
  • EU food contact 2002/72/EC

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183/A
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 in/inISO 294-4
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 71.0 MPaISO 527-2/50
Tensile Strength, Yield 60.0 MPaISO 527-2/50
Elongation at Break 150 %ISO 527-2/50
Elongation at Yield 6.0 %ISO 527-2/50
Tensile Modulus 2300 MPaISO 527-2/50
Flexural Strength 97.0 MPa2.0 mm/min; ISO 178
Flexural Modulus 2400 MPa2.0 mm/min; ISO 178
Izod Impact, Notched (ISO) 88.0 kJ/m²ISO 180/A
Izod Impact, Unnotched (ISO) NBISO 180
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 250 V
@Thickness 2.00 mm
Solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 125 °CIEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 144 °CAnnealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 125 °CUnannealed; ISO 75-2/A
 141 °CAnnealed; ISO 75-2/A
Vicat Softening Point 149 °CISO 306/B50
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 87 - 91 %ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical Lupoy 1201-10 Polycarbonate Resin
RTP Company RTP 300 HF FR A Polycarbonate (PC), High Flow - Unreinforced - Flame Retardant - UL94 V-0
Trinseo CALIBRE™ 200-10 Polycarbonate Resin
Trinseo CALIBRE™ 201-22 Polycarbonate Resin
Trinseo CALIBRE™ 201-6 Polycarbonate Resin

PDWST010 / 142219

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.