MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNTSMAN technical extrusion product range and offers a specially designed, flexible material with a broad processing window particularly suitable in flat die, cast die extrusion processes. IROGRAN A 85 D 5001 DP is a development material.

Performance Features:

  • Excellent wear performance
  • Good processability
  • Antistatic behavior
  • Good melt flow
  • High elasticity

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccInjection molded parts; ASTM D792
Melt Index of Compound 75 g/10 min
@Load 21.6 kg,
Temperature 190 °C
MVR, [cm3/10 min]
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85Injection molded parts; ASTM D2240
Hardness, Shore D 34Injection molded parts; ASTM D2240
Tensile Strength at Break 40.0 MPaInjection molded parts; DIN 53504
Elongation at Break 620 %Injection molded parts; DIN 53504
100% Modulus 0.00500 GPa
@Strain 100 %
Injection molded parts; DIN 53504
300% Modulus 0.0110 GPa
@Strain 300 %
Injection molded parts; DIN 53504
Rebound 36 %Bayshore, Injection molded parts; ASTM D2632
Tear Strength 600 pliInjection molded parts; ASTM D624
Abrasion 25mm3, Injection molded; DIN 53516
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+8 ohmInjection molded parts
 
Processing PropertiesOriginal ValueComments
Feed Temperature 25.0 - 40.0 °CExtrusion
 25.0 - 45.0 °CInjection
Middle Barrel Temperature 180 - 205 °CExtrusion
Nozzle Temperature 185 - 205 °CExtrusion
 185 - 210 °CInjection
Adapter Temperature 180 - 205 °CExtrusion
Die Temperature 185 - 205 °CExtrusion
Mold Temperature 20.0 - 50.0 °CInjection
 
Descriptive Properties
Heating Zone190-210°CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester
Overview of materials for Polyester Thermoplastic Elastomer
Huntsman IROGRAN® A 95 K 4640 TPU-For Seals
Huntsman IROGRAN® D 64 P 4777 TPU-Polyester
Huntsman IROGRAN® PS 370-202 TPU-Polyester

PHUQ092 / 159465

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.