MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 85 E 4607 is a thermoplastic polyether- polyurethane intended for extrusion and injection molding applications. Additional characteristics of the product are excellent mechanical properties and high tear strength.

Performance Features:

  • Good melt flow
  • High wear resistance
  • High elasticity
  • Oil resistance
  • Low-temperature flexibility
Applications: For the production of spiral hoses, tooth belts round cords, casual shoe soles

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inInjection molded; ASTM D955
Melt Index of Compound 35 g/10 min
@Load 21.6 kg,
Temperature 190 °C
35 g/10 min
@Load 47.6 lb,
Temperature 374 °F
MVR, [cm3/10 min]
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585Injection molded parts; ASTM D2240
Hardness, Shore D 3434Injection molded parts; ASTM D2240
Tensile Strength at Break 45.0 MPa6530 psiInjection molded parts; DIN 53504
Elongation at Break 650 %650 %Injection molded parts; DIN 53504
100% Modulus 5.00 MPa
@Strain 100 %
725 psi
@Strain 100 %
Injection molded parts; DIN 53504
300% Modulus 14.0 MPa
@Strain 300 %
2030 psi
@Strain 300 %
Injection molded parts; DIN 53504
Tear Strength 99.9 kN/m570 pliInjection molded parts; ASTM D624
Abrasion 2525mm3, Injection molded; ISO 4649
Compression Set  25 %
@Temperature 22.8 °C,
Time 86400 sec
25 %
@Temperature 73.0 °F,
Time 24.0 hour
Injection molded; ASTM D395
 40 %
@Temperature 70.0 °C,
Time 86400 sec
40 %
@Temperature 158 °F,
Time 24.0 hour
Injection molded; ASTM D395
 
Processing PropertiesMetricEnglishComments
Feed Temperature 25.0 - 40.0 °C77.0 - 104 °FExtrusion
Middle Barrel Temperature 165 - 190 °C329 - 374 °FExtrusion
Nozzle Temperature 170 - 200 °C338 - 392 °FExtrusion
 180 - 200 °C356 - 392 °FInjection
Adapter Temperature 175 - 195 °C347 - 383 °FExtrusion
Die Temperature 175 - 200 °C347 - 392 °FExtrusion
Melt Temperature 170 - 195 °C338 - 383 °FInjection
Mold Temperature 20.0 - 70.0 °C68.0 - 158 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® C 98 A TPUR
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester
Miracll E195 Thermoplastic Polyurethane (TPUR), Polyester Grade
BASF Elastollan® C 85 A HPM TPUR
Covestro Texin® 285 Thermoplastic Polyurethanes (TPU)

PHUQ093 / 159466

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.