MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNTSMAN technical extrusion product range and offers a specially designed, flexible material with a broad processing window particularly suitable in flat die, cast die extrusion processes. IROGRAN A 85 D 5001 DP is a development material.

Performance Features:

  • Excellent wear performance
  • Good processability
  • Antistatic behavior
  • Good melt flow
  • High elasticity

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³Injection molded parts; ASTM D792
Melt Index of Compound 75 g/10 min
@Load 21.6 kg,
Temperature 190 °C
75 g/10 min
@Load 47.6 lb,
Temperature 374 °F
MVR, [cm3/10 min]
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585Injection molded parts; ASTM D2240
Hardness, Shore D 3434Injection molded parts; ASTM D2240
Tensile Strength at Break 40.0 MPa5800 psiInjection molded parts; DIN 53504
Elongation at Break 620 %620 %Injection molded parts; DIN 53504
100% Modulus 5.00 MPa
@Strain 100 %
725 psi
@Strain 100 %
Injection molded parts; DIN 53504
300% Modulus 11.0 MPa
@Strain 300 %
1600 psi
@Strain 300 %
Injection molded parts; DIN 53504
Rebound 36 %36 %Bayshore, Injection molded parts; ASTM D2632
Tear Strength 105 kN/m600 pliInjection molded parts; ASTM D624
Abrasion 2525mm3, Injection molded; DIN 53516
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+8 ohm1.00e+8 ohmInjection molded parts
 
Processing PropertiesMetricEnglishComments
Feed Temperature 25.0 - 40.0 °C77.0 - 104 °FExtrusion
 25.0 - 45.0 °C77.0 - 113 °FInjection
Middle Barrel Temperature 180 - 205 °C356 - 401 °FExtrusion
Nozzle Temperature 185 - 205 °C365 - 401 °FExtrusion
 185 - 210 °C365 - 410 °FInjection
Adapter Temperature 180 - 205 °C356 - 401 °FExtrusion
Die Temperature 185 - 205 °C365 - 401 °FExtrusion
Mold Temperature 20.0 - 50.0 °C68.0 - 122 °FInjection
 
Descriptive Properties
Heating Zone190-210°CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester
Overview of materials for Polyester Thermoplastic Elastomer
Huntsman IROGRAN® A 95 K 4640 TPU-For Seals
Huntsman IROGRAN® D 64 P 4777 TPU-Polyester
Huntsman IROGRAN® PS 370-202 TPU-Polyester

PHUQ092 / 159465

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.