MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Permabond UV640 UV-curable Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PERMABOND UV640 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbonate. Permabond UV640 has very high shear strength, elongation and impact resistance making it ideal for applications that require substrates with different coefficients of thermal expansion. Protect liquid adhesive from room lighting.

Features & Benefits:

  • Cure on demand
  • High shear strength
  • Fast curing with low-power lamps
  • 100% solids, no solvents
  • Excellent adhesion to plastics

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccuncured
Viscosity 3000 - 4000 cP
@Temperature 25.0 °C
Uncured
Storage Temperature 5.00 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60
Tensile Strength 13.0 MPaASTM D2095
Elongation at Break 110 %
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.0
@Frequency 1e+6 Hz,
Temperature 25.0 °C
Dielectric Strength 12.0 kV/mm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -65.0 °F
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.47
 
Processing PropertiesOriginal ValueComments
Cure Time 7.00 secfixture time, (low power 4mW lamp)
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear, colorlessUncured
Cure Wavelength (nm)365-420
Maximum Gap Fill (mm)0.4
Strength Retention10% at 200°CRelative to 0°C
 100% at 0°CRelative to 0°C
 30% at 150°CRelative to 0°C
 75% at 100°CRelative to 0°C
 95% at 50°CRelative to 0°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites LYTEX® 4197 55% Carbon Fiber Reinforced Epoxy SMC
Momentive Performance Materials RTV112 One Component Acetoxy Adhesive Sealant, White
Master Bond EP21TDCF-3 Two Component, Higher Viscosity Epoxy System
Henkel Loctite® Ultra Grey® 5999 Flange Sealant
Henkel Loctite® Nuva-Sil® 5084 Sealant

PPERMA61 / 56169

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.