MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Touchstone CFOAM® 17 Structural Carbon Foam  (discontinued **)
Categories: Carbon; Other Engineering Material; Composite Core Material

Material Notes: CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally insulating or conducting and whose electrical conductivity can be varied over seven orders of magnitude. It can be fabricated in a variety of shapes, sizes, and densities to meet the property requirements of specific applications.

These foams will not off-gas at elevated temperatures and will not support ignition. Unlike most metals and ceramics, CFOAM mechanical properties do not deteriorate with increased temperature if protected from oxidization, making carbon foams an attractive thermal protection material. Carbon foams also are tolerant to impact damage and can be repaired in-place using carbonaceous adhesives. They can be bonded easily to dissimilar materials, such as metals or PMCs, for oxidation or further impact protection, respectively.

Results from ASTM E1354, ASTM E1515, MIL-STD-1623, Coast Guard IMO, and FTP Code Part I and Part III indicate that CFOAM will pass all key fire tests including radiant panel, smoke generation, toxicity, cone calorimeter, fire resistance, and room corner tests.

Information provided by Touchstone Research Laboratory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 17.0 lb/ft³ASTM D1622
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 300 psiASTM C297
Tensile Modulus 50000 psiASTM C297
Compressive Strength 900 psiASTM C365
Compressive Modulus 80000 psiASTM C365
Shear Strength 200 psiTorsional Shear
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0100 - 1.00e+7 ohm-cmTailorable; ASTM D4496
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.70 µin/in-°F
@Temperature 20.0 °C
ASTM E228
Thermal Conductivity 0.250 - 25.0 W/m-KTailorable; ASTM E1225
Maximum Service Temperature, Air 1112 °F
Maximum Service Temperature, Inert 3000 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Touchstone CFOAM® 25 Structural Carbon Foam
Touchstone CFOAM® 20 Structural Carbon Foam
Touchstone CFOAM® 30 Structural Carbon Foam
Cymat A35620SC 020SS Stabilized Aluminum Foam
Destech Open-Celled Glassy Carbon Foam

ETOUCH00 / 6135

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.