MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese FORTRON 309 PPS, Unfilled
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: 0309 exhibits a good balance of flow and melt strength for extrusion processes. The material demonstrates excellent heat and chemical resistance. The intended use of this product is for extruding monofilament/fibers. Available standard in powder (0309B4), pellet (0309P4) and crystallized pellet (0309C4) form.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
Density 1.35 g/ccISO 1183
Water Absorption at Saturation 0.020 %ISO 62
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90ISO 2039-2
 93ASTM D785
Tensile Strength at Break 90.0 MPa5mm/min; ISO 527-2/1A
Elongation at Break 8.0 %5mm/min; ISO 527-2/1A
Flexural Strength 145 MPaISO 178
Flexural Modulus 4200 MPaISO 178
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+7 ohm-cmASTM D257
 1.00e+11 ohm-cmIEC 60093
Dielectric Constant 3.0
@Frequency 1000 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
ASTM D150
 4.6
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 18.0 kV/mmIEC 60243-1
 450 V/milshort term; ASTM D149
Dissipation Factor 0.00090
@Frequency 1e+6 Hz
ASTM D150
 0.0010
@Frequency 1000 Hz
ASTM D150
 0.0011
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 124 secASTM D495
Comparative Tracking Index 125 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 52.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 53.0 µm/m-°CISO 11359-2
Specific Heat Capacity 1.83 J/g-°C
Melting Point 280 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 400 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 115 °CISO 75-1, -2
 220 °FASTM D648
Deflection Temperature at 8.0 MPa 95.0 °CISO 75-1, -2
Glass Transition Temp, Tg 90.0 °CISO 11357-1,-2,-3
 
Processing PropertiesOriginal ValueComments
Processing Temperature 140 - 160 °Ccavity
 310 - 320 °Chot runner
Feed Temperature 60.0 - 80.0 °C
Zone 1 290 - 300 °C
Zone 2 300 - 310 °C
Zone 3 310 - 320 °C
Zone 4 310 - 320 °C
Die Temperature 300 - 310 °C
Melt Temperature 310 - 320 °C
Drying Temperature 110 - 120 °C
Dry Time 3.00 - 4.00 hour
Moisture Content <= 0.020 %
Injection Pressure 40.0 - 80.0 MPa
Hold Pressure 30.0 - 60.0 MPa
Back Pressure <= 3.00 MPa
Screw Speed 50 rpm
@Diameter 55.0 mm
 75 rpm
@Diameter 40.0 mm
 120 rpm
@Diameter 25.0 mm
 
Descriptive Properties
Injection moldingYes
Injection speedfast
Sheet extrusionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese FORTRON 203 PPS, Unfilled
Celanese FORTRON 205 PPS, Unfilled
Celanese FORTRON 320 PPS, Unfilled
Celanese FORTRON 214 PPS, Unfilled
Celanese FORTRON 0203HS PPS, Unfilled

PHCQ262 / 178717

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.