MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Covestro Bayblend® MTR Extruded Thermoplastic
Categories: Polymer; Thermoplastic

Material Notes: Bayblend® MTR sheet is an opaque product offering a combination of low flammability characteristics, robust mechanical properties, and ease of fabrication. Bayblend MTR complies with the flammability and smoke emission requirements for transit materials per the U.S. Federal Railroad Administration, listed in DOT: 49 CFR 238, and meets the criteria in the Bombardier Transportation Standard SMP 800-C for Toxic Gas Generation. Bayblend MTR has lower specific gravity, higher stiffness, higher strength, and greater toughness than typical non-metallic materials used for mass transportation interior components. This combination of physical properties allows for design of thinner and lighter parts that often do not require secondary reinforcement or stiffeners. Bayblend MTR is available in a variety of textures and colors.

Applications: Thermoformed rail interior parts such as seating components, wall cladding, window reveals, and ceiling panels

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D792
Moisture Absorption at Equilibrium 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 6060ASTM D785
Hardness, Rockwell R 116116ASTM D785
Tensile Strength at Break 49.0 MPa7110 psiASTM D638
Tensile Strength, Yield 54.5 MPa7900 psiASTM D638
Elongation at Break 11 %11 %ASTM D638
Modulus of Elasticity 3.72 GPa540 ksiASTM D638
Flexural Strength 103 MPa14900 psiASTM D790
Flexural Modulus 3.65 GPa529 ksiASTM D790
Izod Impact, Notched 0.801 J/cm
@Thickness 3.00 mm
1.50 ft-lb/in
@Thickness 0.118 in
ASTM D256
Impact Test 27.1 J
@Thickness 3.00 mm
20.0 ft-lb
@Thickness 0.118 in
ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  4.00e+15 ohm-cm
@Thickness 2.84 mm
4.00e+15 ohm-cm
@Thickness 0.112 in
ASTM D257
 6.60e+15 ohm-cm
@Thickness 3.17 mm
6.60e+15 ohm-cm
@Thickness 0.125 in
ASTM D257
Dielectric Constant  2.9
@Thickness 3.00 mm,
Frequency 1e+6 Hz
2.9
@Thickness 0.118 in,
Frequency 1e+6 Hz
ASTM D150
 3.0
@Thickness 3.17 mm,
Frequency 60 Hz
3.0
@Thickness 0.125 in,
Frequency 60 Hz
ASTM D150
Dielectric Strength 24.2 kV/mm615 kV/inASTM D149
Dissipation Factor  0.0040
@Thickness 3.17 mm,
Frequency 1e+6 Hz
0.0040
@Thickness 0.125 in,
Frequency 1e+6 Hz
ASTM D150
 0.0060
@Thickness 3.00 mm,
Frequency 60 Hz
0.0060
@Thickness 0.118 in,
Frequency 60 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 49.1 µm/m-°C27.3 µin/in-°FASTM D696
Thermal Conductivity 1.92 W/m-K13.3 BTU-in/hr-ft²-°FASTM E1530
Insulation R Value 0.900.90Btu-ft2-hr°F; ASMT E1530
Deflection Temperature at 0.46 MPa (66 psi) 103 °C217 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 96.1 °C205 °FASTM D648
Vicat Softening Point 111 °C232 °FASTM D1525
Smoke Density 1.5 min1.5 min<100; ASTM D622
 4.0 min4.0 min<200; ASTM E622

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Stanyl® TW363 PA46, Conditioned, Heat Stabilized, Impact Modified
Covestro Bayblend® FR411 MT PC Blend
Covestro Bayblend® CG100 PC/ABS Blend
Envalior Stanyl® TW363 (COND) Nylon 46 Heat Stabilized, Impact Modified (North America)
Covestro Bayblend® W90 XG PC/ABS Blend

PCOVEST0039 / 201822

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.