MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Covestro Bayblend® MTR Extruded Thermoplastic
Categories: Polymer; Thermoplastic

Material Notes: Bayblend® MTR sheet is an opaque product offering a combination of low flammability characteristics, robust mechanical properties, and ease of fabrication. Bayblend MTR complies with the flammability and smoke emission requirements for transit materials per the U.S. Federal Railroad Administration, listed in DOT: 49 CFR 238, and meets the criteria in the Bombardier Transportation Standard SMP 800-C for Toxic Gas Generation. Bayblend MTR has lower specific gravity, higher stiffness, higher strength, and greater toughness than typical non-metallic materials used for mass transportation interior components. This combination of physical properties allows for design of thinner and lighter parts that often do not require secondary reinforcement or stiffeners. Bayblend MTR is available in a variety of textures and colors.

Applications: Thermoformed rail interior parts such as seating components, wall cladding, window reveals, and ceiling panels

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Moisture Absorption at Equilibrium 0.10 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 60ASTM D785
Hardness, Rockwell R 116ASTM D785
Tensile Strength at Break 49.0 MPaASTM D638
Tensile Strength, Yield 54.5 MPaASTM D638
Elongation at Break 11 %ASTM D638
Modulus of Elasticity 3.72 GPaASTM D638
Flexural Strength 103 MPaASTM D790
Flexural Modulus 3650 MPaASTM D790
Izod Impact, Notched 1.50 ft-lb/in
@Thickness 3.00 mm
ASTM D256
Impact Test 20.0 ft-lb
@Thickness 3.00 mm
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+15 ohm-cm
@Thickness 2.84 mm
ASTM D257
 6.60e+15 ohm-cm
@Thickness 3.17 mm
ASTM D257
Dielectric Constant 2.9
@Thickness 3.00 mm,
Frequency 1e+6 Hz
ASTM D150
 3.0
@Thickness 3.17 mm,
Frequency 60 Hz
ASTM D150
Dielectric Strength 24.2 kV/mmASTM D149
Dissipation Factor 0.0040
@Thickness 3.17 mm,
Frequency 1e+6 Hz
ASTM D150
 0.0060
@Thickness 3.00 mm,
Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 27.3 µin/in-°FASTM D696
Thermal Conductivity 13.3 BTU-in/hr-ft²-°FASTM E1530
Insulation R Value 0.90Btu-ft2-hr°F; ASMT E1530
Deflection Temperature at 0.46 MPa (66 psi) 103 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 96.1 °CASTM D648
Vicat Softening Point 111 °CASTM D1525
Smoke Density 1.5 min<100; ASTM D622
 4.0 min<200; ASTM E622

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Stanyl® TW363 PA46, Conditioned, Heat Stabilized, Impact Modified
Covestro Bayblend® FR411 MT PC Blend
Covestro Bayblend® CG100 PC/ABS Blend
Envalior Stanyl® TW363 (COND) Nylon 46 Heat Stabilized, Impact Modified (North America)
Covestro Bayblend® W90 XG PC/ABS Blend

PCOVEST0039 / 201822

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.