MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 221 Natural FA PA66, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Description: Product in development. Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. Suitable for food contact applications

Available in: Europe and North America

Product Applications: TECHNYL® A 221 NATURAL FA offers a good combination between primary properties of the unreinforced polyamide 66 and processing properties leading to increased productivity. These performances are associated with excellent dimensional stability and good rigidity of molded parts. This grade is used in a wide variety of industries: Automotive: connectors, Electrical: connectors, rotary switches and Consumer goods: lighters, aerosol valves. This product is available in natural.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183/A
Water Absorption 1.1 %ISO 62
Linear Mold Shrinkage 0.0082 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0127 cm/cm
Linear Mold Shrinkage, Transverse 0.0155 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 95.0 MPaISO 527 Type 1A
Elongation at Break 20 %ISO 527 Type 1A
Tensile Modulus 3200 MPaISO 527 Type 1A
Flexural Strength 140 MPaISO 178
Flexural Modulus 3300 MPaISO 178
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 2.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CISO 75/Af
 
Processing PropertiesOriginal ValueComments
Feed Temperature 250 - 270 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone260-280°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 205F PA66, DRY
Domo TECHNYL® A 217 PA66, DRY
Domo TECHNYL® A 221 PA66, DRY
Domo TECHNYL® A 221 Natural FA PA66, Conditioned
Domo TECHNYL® A 216 NATURAL FA PA66, DRY

PRHOD683 / 137914

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.