MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kaneka Kane Ace MX-701 BMI
Categories: Polymer; Thermoset

Material Notes: 33% concentration of PBd CSR particles in a tri-functional polyol (BASF Pluracol 858) for use in polyurethane applications

Information provided by Kaneka North America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 10000 cP
@Temperature 25.0 °C
 
Descriptive Properties
Carrier ResinPluroacol 858
CSR32-34%
CSR Size200 nm
CSR TypePBd
Inhibitor LevelOH 620

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vyncolit Neopreg Kinel® SK4503 S5 Aramid Reinforced Molding Compound
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin
Henkel Hysol EA 9833.1 (BMI) Core Splice Adhesive
Henkel Hysol EA 9673 (BMI) Film Adhesive
Evonik Compimide® TM124-ether 2,2'-Bis(4-allyloxyphenyl)propane

PKANEKA836 / 183775

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.