MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® 353ND Black High Temperature Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, High Temperature

Material Notes: Product Description: EPO TEK® 353ND Black is a a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applications

Advantages & Application Notes:

  • EPO TEK® 353ND-BLACK has been color-coded black for optical applications requiring opacity against light in IR and VIS region.
  • Reasonable pot-life that allows for low temperature curing to be realized.
  • Semiconductor suggested applications: wafer-wafer bonding of CSP; fabrication of MEMs devices; flip chip underfill.
  • Hybrid suggested applications: providing near hermetic seals in sensor devices, resisting high temperature packaging.
  • Fiber optic adhesive designed to meet Telecordia 1221 - suggested applications:
    • Sealing fiber into ferrules, transmitting light in the optical pathway from 800- 1550 nm range
    • Fiber component packaging; adhesive for active alignment of optics, environmental seal of opto-package, V-groove arrays
    • Down-Hole petrochemical fiber optic sensors, resisting >200 C field conditions
  • Medical suggested applications:
    • Potting Fiber Optic bundles into SST ferrules for light guides and endoscopes, resisting sterilization cycles of autoclave, ETO, gamma, H202 plasma
  • Electronics Assembly suggested applications:
    • Used as dielectric layer in the fabrication of capacitors; laminating PZT ferroelectrics found in ultrasound or ink-jetting devices
    • Impregnating and insulating copper coil windings in motors and inductor coils. Bonding ferrite cores and magnets
    • Structural grade epoxy found in hard-disk drive devices; bonding of SST metals, kapton, and magnets

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccPart B
 1.22 g/ccPart A
Viscosity 3000 - 5000 cP
@Temperature 23.0 °C
50 rpm
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Na (Sodium) 52 ppm
Ionic Impurities - K (Potassium) 16 ppm
Ionic Impurities - Cl (Chloride) 595 ppm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
Tensile Modulus 517000 psiStorage
Shear Strength >= 2000 psiLap
 >= 5100 psiDie
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.60e+13 ohm-cm
Dielectric Constant 3.09
@Frequency 1000 Hz
Dissipation Factor 0.0050
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 54.0 µm/m-°CBelow Tg
 206 µm/m-°CAbove Tg
Maximum Service Temperature, Air 225 °CContinuous
 325 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 90.0 °CDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 420 °CDegradation Temperature
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 min
@Temperature 150 °C
Minimum Bond Line
 5.00 min
@Temperature 120 °C
Minimum Bond Line
 10.0 min
@Temperature 100 °C
Minimum Bond Line
 30.0 min
@Temperature 80.0 °C
Minimum Bond Line
Pot Life 180 - 240 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
 
Descriptive Properties
ColorAmberPart B
 BlackPart A
ConsistencyPourable liquid
Ionic Impurities NH41149 ppm
Mix Ratio by Weight10:1
Number of ComponentsTwo
Weight Loss0.92%200°C
 1.24%250°C
 1.83%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 353ND High Temperature Epoxy
Epoxy Technology EPO-TEK® H62 Thermally Conductive Epoxy
Epoxy Technology EPO-TEK® 920-FL Thermally Conductive Epoxy
Epoxy Technology EPO-TEK® 509FM-1 General Purpose Epoxy
Epoxy Technology EPO-TEK® 353ND-T1 High Temperature Thixotropic Epoxy

PPOXYT123 / 141162

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.