MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Goodfellow Aluminum 99/Silicon 1 Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: An addition of 1% Silicon lowers the melting range without producing brittleness. Aluminum/Silicon alloys are used in brazing alloys and welding wire for joining Aluminum as well as bonding wire in the semi-conductor industry.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.70 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 310 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000260 - 0.00000350 ohm-cmTemperature Coefficient of 0.0042/K
 
Thermal PropertiesOriginal ValueComments
Melting Point 600 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 99 %
Silicon, Si 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alpase M-5™ Aluminum Mold Plate
Arkema Kynar Flex® 2801-00 Polyvinylidene Fluoride Powder
Arkema KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Constellium DOKIMA® Rolled Plate Aluminum
LG Chemical MA201 ABS, Low Gloss

NGOODF112 / 16196

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.