MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Johnson Matthey Silver-flo™ 452 Cadmium Free Silver Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Silver-flo™ 452 is a cadmium free silver brazing filler metal. It exhibits a comparatively low brazing temperature with a short melting range. Silver-flo™452 is relatively free flowing and produces neat joints with small fillets.

This filler metal has been used for brazing of PCD segments in tool applications. In these cases the brazing temperature has successfully been kept below the point at which the PCD begins to degrade.

It should be noted that this filler metal contains tin and may be described as being ‘hot-short’. It should not be quenched from high temperatures (in excess of 300°C) and care should be taken when it is used to braze components with widely differing coefficients of thermal expansion as in both cases cracking of the joints may occur.

Silver-flo 452™ is recommended where the presence of silicon is not desirable. This alloy is suitable for seawater applications, being resistant to dezincification.

This filler metal can be used to join all the common engineering materials (excluding aluminum) – such as copper, copper alloys (including, brasses, bronzes, gun metal, nickel silvers, aluminum bronze, copper nickel) and steel (including, mild, carbon, tool steel, stainless steels and low alloy steel). It may be used for brazing tungsten carbide and PCD segments however where cracking of the carbide or wetting of the filler metal may be an issue specialized silver brazing filler metals containing nickel / manganese are often preferred.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 640 - 680 °C
Solidus 640 °C
Liquidus 680 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 27 %
Silver, Ag 45 %
Tin, Sn 2.5 %
Zinc, Zn 25.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Johnson Matthey Silver-flo™ 56 Cadmium Free Silver Brazing Paste
NBE nanoTach® Nano-Silver Paste, Lead-Free Solder Alternative
Aremco Pyro-Duct™ 597-A Electrically & Thermally Conductive Material, Silver Filled
AISI 1008 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round
Johnson Matthey Pallabraze™ 1179 Precious Metal Brazing Filler Metal

NJMMJ9780 / 186181

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.