MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
VICTREX HT™ P45 Polyetherketone
Categories: Polymer; Thermoplastic; Polyketone

Material Notes: Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion compounding, low flow, FDA food contact compliant, colour natural.

Information Provided by Victrex.

Key Words: PEK
Vendors: Victrex is a global leader in high-performance PEEK and PAEK polymers, transforming industries from aerospace to medical devices. For 40 years, our innovative polymer solutions help customers achieve new levels of performance, sustainability, and cost efficiency across applications that millions rely on daily from smartphones to aircraft components. As pioneers in polymer engineering, we're committed to delivering transformational solutions that address global materials challenges. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccCrystalline; ISO 1183
Viscosity 350000 cP
@Temperature 400 °C
Melt; ISO 11443
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 100 MPaISO 527
Elongation at Break 15 %ISO 527
Tensile Modulus 4.20 GPaISO 527
Flexural Strength 170 MPaISO 178
Flexural Modulus 4.20 GPaISO 178
Izod Impact, Notched (ISO) 6.50 kJ/m²ISO 180/A
Izod Impact, Unnotched (ISO) NBISO 180/U
 
Thermal PropertiesOriginal ValueComments
Melting Point 373 °CISO 11357
Glass Transition Temp, Tg 152 °COnset; ISO 11357
 160 °CMidpoint
 
Processing PropertiesOriginal ValueComments
Processing Temperature 400 - 420 °C
Dry Time 3.00 hour
@Temperature 150 °C
 5.00 hour
@Temperature 120 °C
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
VICTREX™ WG101 Polyaryletherketone
Lehvoss LUVOCOM® 70-9113/BK Polyketone with PTFE, lubricant modified, easy flowing, demolding aid
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material
Saint-Gobain Meldin® 5320 Thermoplastic Bearing Material

PVICTB10 / 122198

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.