MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik CYREX® Protect Acrylic-polycarbonate alloy
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic/Polycarbonate Alloy

Material Notes: CYROLITE® Protect and CYROLITE® Protect 2 acrylic-based multipolymer compounds and CYREX® Protect acrylic-polycarbonate alloy provide antimicrobial capabilities* against a variety of microorganisms commonly found in healthcare facilities. Antimicrobial products are used in medical devices for secondary infection management or to inhibit bacterial growth.

Benefits:

  • Antimicrobial capabilities within the polymer structure. No secondary operations required.
  • Chemical resistance to lipids and alcohol
  • Easily welded
  • Bondable to PVC tubing
  • Excellent impact strength
  • EtO, gamma and e-beam sterilizable
Opaque medical white color, outstanding impact resistance and toughness, excellent resistance to lipids and alcohol and higher heat resistance

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 3.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
3.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 54.4 MPa7890 psiASTM D638
Elongation at Break 25 %25 %ASTM D638
Elongation at Yield 4.0 %4.0 %ASTM D638
Tensile Modulus 2.14 GPa310 ksiASTM D638
Flexural Strength 92.4 MPa13400 psiASTM D790
Flexural Modulus 2.10 GPa305 ksiASTM D790
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Thickness 6.35 mm,
Temperature 23.0 °C
5.71 ft-lb/in²
@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 130 °C266 °FASTM D648
Vicat Softening Point 130 °C266 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 243 - 266 °C469 - 511 °F
Mold Temperature 65.0 - 99.0 °C149 - 210 °F
Drying Temperature 82.0 °C180 °FPredrying
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourPredrying

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm CyRex® 100 Acrylic-Polycarbonate Alloy
Evonik CYROLITE® Protect Acrylic-polycarbonate alloy
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant
Röhm CyRex® 400 Acrylic-Polycarbonate Alloy
RTP Company RTP 1800 A FR Polycarbonate/Acrylic Alloy (PC/PMMA), Flame Retardant - UL94

PEVONIL075 / 196279

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.