MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik CYREX® Protect Acrylic-polycarbonate alloy
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic/Polycarbonate Alloy

Material Notes: CYROLITE® Protect and CYROLITE® Protect 2 acrylic-based multipolymer compounds and CYREX® Protect acrylic-polycarbonate alloy provide antimicrobial capabilities* against a variety of microorganisms commonly found in healthcare facilities. Antimicrobial products are used in medical devices for secondary infection management or to inhibit bacterial growth.

Benefits:

  • Antimicrobial capabilities within the polymer structure. No secondary operations required.
  • Chemical resistance to lipids and alcohol
  • Easily welded
  • Bondable to PVC tubing
  • Excellent impact strength
  • EtO, gamma and e-beam sterilizable
Opaque medical white color, outstanding impact resistance and toughness, excellent resistance to lipids and alcohol and higher heat resistance

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 3.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 54.4 MPaASTM D638
Elongation at Break 25 %ASTM D638
Elongation at Yield 4.0 %ASTM D638
Tensile Modulus 2140 MPaASTM D638
Flexural Strength 92.4 MPaASTM D790
Flexural Modulus 2.10 GPaASTM D790
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Thickness 6.35 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 130 °CASTM D648
Vicat Softening Point 130 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 243 - 266 °C
Mold Temperature 65.0 - 99.0 °C
Drying Temperature 82.0 °CPredrying
Dry Time 3.00 - 4.00 hourPredrying

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm CyRex® 100 Acrylic-Polycarbonate Alloy
Evonik CYROLITE® Protect Acrylic-polycarbonate alloy
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant
Röhm CyRex® 400 Acrylic-Polycarbonate Alloy
RTP Company RTP 1800 A FR Polycarbonate/Acrylic Alloy (PC/PMMA), Flame Retardant - UL94

PEVONIL075 / 196279

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.