MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
RSP Technology RSA-462 T6 Aluminum Super Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: Pistons, precision equipment, high strength-high temperature; Specifically developed for racing pistons

Features: High strength and fatigue at elevated temperatures (150 - 450C), low density, low CTE, high stiffness, Good wear resistance

Applications:

  • racing pistons for micro engines, 2-strokes, 4-strokes
  • precision equipment combining high strength, high stiffness and low CTE
Replacing: conventional AA4032, AA2618, M-142, titanium

RSP Technology develops, produces and sells aluminium super alloys with high end properties. By using its own Meltspinning process, ultra fast cooling rates can be reached, converting more than 1 million degrees per second. As a result very fine nanostructured alloys with new functionalities are being developed and produced.

Information provided by RSP Technology BV

Vendors: RSP Technology – Aluminum as strong as Titanium For more information contact: +31 (0)596 632 300 or visit www.rsp-technology.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.63 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 185
Tensile Strength, Ultimate 470 MPa
 135 MPa
@Temperature 300 °C,
Time 1800 sec
 250 MPa
@Temperature 250 °C,
Time 1800 sec
 345 MPa
@Temperature 200 °C,
Time 1800 sec
 410 MPa
@Temperature 150 °C,
Time 1800 sec
 460 MPa
@Temperature 100 °C,
Time 1800 sec
Tensile Strength, Yield 420 MPa
Elongation at Break 2.5 %
 5.0 %
@Temperature 250 °C
Tensile Modulus 90.0 GPa
Fatigue Strength 100 MPa
@Temperature 250 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.8 µm/m-°C
Thermal Conductivity 130 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 72.5 %
Copper, Cu 1.5 %
Iron, Fe 0.40 %
Magnesium, Mg 1.2 %
Nickel, Ni 0.40 %
Silicon, Si 24 %
 
Descriptive Properties
Specific Fatigue117%AA 2618 = 100%
Specific Stiffness34GPa/(g/cc)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RSP Technology RSA-443 AE Aluminum Super Alloy
RSP Technology RSA-444 T6 Aluminum Super Alloy
RSP Technology RSA-461 T6 Aluminum Super Alloy
RSP Technology RSA-4019 AE Aluminum Super Alloy
RSP Technology RSA-6061 T6 Aluminum Super Alloy

NRSP26 / 100840

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.