MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond EP21LSCL-1 Two Component, Room Temperature Curing Epoxy Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Description: Master Bond Polymer System EP21LSCL-1 is a two component, low viscosity epoxy resin system featuring optical clarity as well as non-yellowing properties. This system can be used for high performance coating, bonding, sealing, encapsulation and casting. It is formulated to cure easily at room temperature or more quickly at elevated temperatures. Master Bond EP21LSCL-1 is 100% reactive and does not contain any solvents or volatiles. It bonds well to metals, glass, ceramics, wood and many plastics and has good chemical resistance to water, fuels, oils, acids and bases. EP21LSCL-1 has great electrical insulation properties. Also of great significance is EP21LSCL-1’s exceptionally long open time. This low exothermic epoxy is ideal for larger castings ranging upwards of 2-3 inches thick. Its service temperature range is from -60°F to +250°F. It has excellent clarity and light transmission and unlike most epoxy formulations, it has very good clarity retention.

Product Advantages:

  • Simple 100:60 mix ratio by weight.
  • Low viscosity; easily applied for bonding, sealing, coating and encapsulating.
  • Long working life.
  • Excellent physical strength properties, and good chemical resistance.
  • Adhesion to similar and dissimilar substrates.
  • Non-yellowing characteristics.
  • Electrical insulation properties.Information provided by MasterBond®
Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 600 - 1200 cP600 - 1200 cPPart B
 1800 - 2500 cP1800 - 2500 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 75>= 75
Tensile Strength at Break >= 62.1 MPa
@Temperature 23.9 °C
>= 9000 psi
@Temperature 75.0 °F
Tensile Modulus 2.41 - 2.76 GPa
@Temperature 23.9 °C
350 - 400 ksi
@Temperature 75.0 °F
Shear Strength >= 13.8 MPa>= 2000 psiAl/Al, Tensile lap
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cm
Dielectric Constant 4.14.1
Dielectric Strength 17.3 kV/mm
@Thickness 3.17 mm
440 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 - 45.0 µm/m-°C22.2 - 25.0 µin/in-°F
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  180 min
@Temperature 93.3 °C
3.00 hour
@Temperature 200 °F
 180 - 300 min
@Temperature 23.9 °C
3.00 - 5.00 hour
@Temperature 75.0 °F
Pot Life 9.0 - 11 min9.0 - 11 min100 gram mass
Shelf Life 12.0 Month
@Temperature 23.9 °C
12.0 Month
@Temperature 75.0 °F
in original closed containers
 
Descriptive Properties
90% gloss retention2000 hrsXenon Weather-O-Meter
 400 hrsQUV Cyclic Ultraviolet Weathering Tester
Mixing Ratio (A to B)100:60by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP112M Two Component, Medium Viscosity Heat Curing Cycloaliphatic Epoxy Resin
Hexcel® HexPly® F155 Epoxy Resin
Master Bond EP21SC-1 Two Component Epoxy Resin System
Solvay CYCOM® 7701 Epoxy - Crowfoot Satin Fabric Composite
Hexcel® F161 Epoxy Resin

PMASTB312 / 149559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.