MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond MasterSil 415 One Component Room Temperature Curing, Transparent Silicon
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Key Features:
  • Extraordinary low temperature serviceability
  • Room temperature cure
  • Easy to handle
  • Outstanding optical clarity
Product Description: MasterSil 415 is a one component acetoxy type, high performance silicone for bonding and sealing. It has a paste consistency and a non-drip application feature. MasterSil 415 is special in that it has excellent optical clarity along with superior non-yellowing properties. Also noteworthy is its low temperature serviceability; the range being from -185°F to +400°F. It bonds well to a wide variety of substrates such as glass, metals, many plastics, composites and various rubber materials including silicone. It is a faster curing system, although the speed is dependent on the thickness of the layer and the level of humidity. As a one part silicone, it has superb elasticity and flexibility. Also, it is a reliable electrical insulator. MasterSil 415 can be used in a wide variety of applications, particularly when silicone type flexibility along with low temperature serviceability and/or transparency are desirable.

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 25 - 3525 - 35
Tensile Strength 2.07 - 2.76 MPa300 - 400 psi
Elongation at Break 350 - 450 %350 - 450 %
Adhesive Bond Strength 2.07 - 2.41 MPa300 - 350 psiTensile Lap, Aluminum to Aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 2.5
@Frequency 60 Hz
2.5
@Frequency 60 Hz
Dielectric Strength 19.7 kV/mm
@Thickness 3.17 mm
500 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -121 °C-185 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 720 - 1440 min12.0 - 24.0 hour
Tack-Free Time 5.00 - 10.0 min0.0833 - 0.167 hour>50% humidity 0.10” thick
Shelf Life 6.00 Month
@Temperature <=23.9 °C
6.00 Month
@Temperature <=75.0 °F
in original, unopened containers
 
Descriptive Properties
Colorclear
Viscositypaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials TSE3033 Clear General Purpose Potting/Encapsulating Compound
Lord Adhesives Thermoset™ SC-300M Silicone Gel Encapsulant
3M Scotchcast™ 2123 Re-enterable Insulating Electrical Resin
Henkel Loctite® Shadowcure™ 5293 Silicone Coating
Henkel Loctite® Output™ 5404 Heat Cure Silicone

PMASTM933 / 185526

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.