MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.

Benefits: This grade shows an outstanding retention of properties after long term ageing in automotive cooling liquids, in comparison with standard glycol grade TECHNYL® A 218 V30 black 34NG.

Available in: Europe

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: Cooling and heating radiator systems, header tanks, thermostat components, inlet & outlet pipes…

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183/A
Water Absorption 0.80 %
@Temperature 23.0 °C,
Time 86400 sec
0.80 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0062 cm/cm0.0062 in/inIsotropy
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 195 MPa28300 psiISO 527 Type 1A
Elongation at Break 3.0 %3.0 %ISO 527 Type 1A
Tensile Modulus 10.0 GPa1450 ksiISO 527 Type 1A
Flexural Modulus 9.20 GPa1330 ksiISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched 8.70 J/cm²41.4 ft-lb/in²ISO 179/1eU
 6.70 J/cm²
@Temperature 135 °C,
Time 720000 sec
31.9 ft-lb/in²
@Temperature 275 °F,
Time 200 hour
after aging water/glycol; ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
11.1 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 263 °C505 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75/Af
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
1210
 
Processing PropertiesMetricEnglishComments
Feed Temperature 260 - 270 °C500 - 518 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY
Domo TECHNYL® A 218 PA66, 33% glass fiber, DRY
Domo TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, Conditioned
Domo Technyl® C216V30 30% Glass Filled Nylon 6
EMS-Grivory Grilon® TSG-30/4 W PA666-GF30

PRHOD668 / 137899

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.