MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Goodfellow Polyacrylamide/acrylate Hydrogel
Categories: Polymer; Thermoplastic

Material Notes: A copolymer of acrylamide and acrylic acid (normally supplied as the sodium salt) that is cross-linked sufficiently to render it insoluble in water but which retains its hydrophilic nature. It therefore can absorb a very large amount of water, swelling proportionately as it does so. The amount of water that can be absorbed is typically around 400x the weight of polymer if the water is completely free of solutes, decreasing quite markedly as the level of solute(s) increases.

Its applications include horticulture, hygiene products like disposable diapers and inummerable odd jobs around the laboratory.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/cc
 
Descriptive Properties
Chemical Resistance - AlcoholsGood
Chemical Resistance - AlkalisFair
Chemical Resistance - AromaticsGood
Chemical Resistance - Dilute AcidsGood-Fair
Chemical Resistance - HalogensGood
Chemical Resistance - KetonesGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CMT Materials METAPOR® BF 100 AL Air Permeable Material
CMT Materials PROTOBLOCK Air Permeable Prototype Tooling Material
CMT Materials METAPOR® HD 210 AL Air Permeable Material
Lubrizol LifeSciences Tecophilic® TG-500 Hydrophilic TPU Hydrogel
BASF Ecoflex® C1200 F Blend Biodegradable Polyester

PGOODF211 / 42282

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.