MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay RHODOLINE® 286N Surfactant
Categories: Fluid

Material Notes: Description: Hydrophilic copolymer dispersant. Semi gloss to high gloss, TiO2 slurry, interior/exterior, low foam.

Identification: AMMONIUM POLYACRYLATE COPOLYMER SOLUTION

Available in: North America

Applications: RHODOLINE© 286N is an acrylic, non-foaming, multi-purpose anionic dispersant. Use RHODOLINE© 286N at concentration of 2 to 8 pounds per 100 gallons of finished paint. The optimum use level of RHODOLINE© 286N in each formulation may be determined by running a dispersant demand curve.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/cc
Solids Content 49 - 51 %
@Temperature 130 °C,
Time 3600 sec
Oven, 0.5 g; RP-0540
Volatile Organic Compounds (VOC) Content <= 1.0 g/lASTM D2369
pH 6.5 - 7.3RP-0420
Viscosity 50 - 200 cP#2 sp @ 30 rpm; RP-0596
Molecular Weight 2700 g/mol
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceClear, Colorless to yellowRP-0064

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Omya OMYACARB® 10 - LU Calcium Carbonate
Solvay RHODOLINE® 622 Surfactant
ExxonMobil Optema® TC-110 Molding Ethylene Methyl Acrylate
ExxonMobil Metallyte™ 100 MET OPP Film
ExxonMobil Ethylene Methyl Acrylate, Extrusion Coating Grade

WRHOD476 / 137707

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.