MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nabaltec ACTILOX® 200 AS1 AlO(OH) Boehmite
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Surface treated flame retardant filler with reduced particle size and optimized viscosity in engineering plastics for synergistic effects with other flame retardants.

Properties:

  • Very fine product in parallel with low spec. surface area
  • Very low viscosity
  • High chemical purity
  • Low electrolyte content
  • Acid scavenger
  • Excellent polymer compatibility

Information provided by Nabaltec.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.230 g/cc0.00831 lb/in³
Brightness 97 %
@Wavelength 457 nm
97 %
@Wavelength 457 nm
Whiteness; Elrepho
Oil Absorption 36 %36 %(ml/100 g)
Moisture Absorption at Equilibrium 0.60 %0.60 %
Loss On Ignition 18 %18 %
Particle Size 0.35 µm0.35 µmMedian
Specific Surface Area 18 m²/g18 m²/gBET
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 33
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 33333 ohm-cm33333 ohm-cm
 
Descriptive Properties
Aluminum Hydroxide (%)99.7
Sieve Analysis0.003%> 45 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical MP220 ABS, High Adhesion, Heat Resistance
BASF Ultraform® N2320 006 POM
Polyplastics TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC)
Nabaltec ACTILOX® B60 AS1 AlO(OH) Boehmite
Aremco Pyro-Paint™ 634-AS-1 High Temperature Refractory Coating

CNABAL27F / 159809

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.