MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Honeywell ACLAR® 22A (2.00 mil) Copolymer Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Fluoropolymer

Material Notes: Description: ACLAR® 22A is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It is a flexible transparent film used to package moisture sensitive products.

Information provided by Honeywell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.08 g/ccASTM D1505
Density 0.0750 lb/in³Yield Density
Water Vapor Transmission 0.300 g/m²/day
@Temperature 37.8 °C
100%RH; ASTM F1249
Thickness 2.00 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 115 - 225 %ASTM D882
Film Elongation at Break, TD 200 - 300 %ASTM D882
Secant Modulus, MD 0.965 - 1.103 GPaASTM D882
Secant Modulus, TD 1.034 - 1.103 GPaASTM D882
Tear Strength Test 250 - 325graves tear TD, grams/mil; ASTM D1004
 325 - 350graves tear MD, grams/mil; ASTM D1004
Film Tensile Strength at Break, MD 7500 - 11000 psiASTM D882
Film Tensile Strength at Break, TD 5000 - 8000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.000530 cal cm/sec-cm²-°C
Melting Point 190 °Ccrystalline melting point; ASTM D4591
Oxygen Index 100 %ASTM D2863
Shrinkage, MD 12 - 15 %
@Treatment Temp. 149 °C,
Time 601 sec
ASTM D1204
Shrinkage, TD -15.0 - -12.0 %
@Treatment Temp. 149 °C,
Time 601 sec
ASTM D1204
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D1003
Transmission, Visible 90 %transparent; thickness not quantified
 
Descriptive Properties
Flammabilitynon flammable

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® WC Polyester Film, 75 Gauge
ExxonMobil LDPE LD 306.75 Low Density Polyethylene Resin
DuPont™ Kapton® 200ZT Polyimide Film, 50 Micron Thickness
DuPont Teijin Films Mylar® OL2 Polyester Film, 75 Gauge
DuPont Teijin Films Mylar® MDA Polyester Film, 75 Gauge

PALA52 / 23144

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.