MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
American Maple, Rock (Sugar Maple)
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: High resistance to abrasion. Diffuse-Porous Hardwood. Least easy to work with hand tools. Excellent shaping, fair planing, fair steam bending. Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Fine
Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium
Resistance to fungal decay (Heartwood in ground contact): Non-durable (5 to 10 years)
Resistance to penetration by preservatives: Resistant
Common Applications: Excellent flooring timber. Furniture. Sports goods

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Acer saccharum; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.570 g/ccOven Dry Weight/Unseasoned Volume
 56.0 lb/ft³Unseasoned*
Cell Length 0.800 mmMature Wood
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 4000 NSide. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 4400 NEnd. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 6400 NSide
Tensile Strength, Ultimate 770 psiPerpendicular to Grain*
Modulus of Rupture 0.109 GPaIn Bending
 9.10 ksiStatic Bending*
Flexural Yield Strength 65.5 MPaBending stress at proportional limit
 5000 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 12.4 - 12.63 GPaIn Bending
 1480 ksiStatic Bending*
Compressive Strength 12.5 MPaPerpendicular to Grain
 53.8 - 54.0 MPaParallel to Grain
 750 psiPerpendicular to Grain*
 3120 psiParallel to Grain*
 3860 psiMax Crushing Strength Parallel to Grain*
Poissons Ratio 0.037µTL, 12% Moisture Content
 0.065µRL, 12% Moisture Content
 0.349µTR, 12% Moisture Content
 0.424µLR, 12% Moisture Content
 0.476µLT, 12% Moisture Content
 0.774µRT, 12% Moisture Content
Machinability 50 %Medium Relative to Other Wood
Shear Strength 16.1 MPaOrientation Unknown
 1380 psiParallel to Grain*
Impact 5.0in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 12100psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 1.08 in-lb/in³Static Bending*
Work to Maximum Load 11.9 in-lb/in³Static Bending*
Toughness 40.7 JTangential
 41.8 JRadial
Cleavage 66.0 kN/mRadial surface of failure, Unseasoned*
 90.0 kN/mTangential surface of failure, Unseasoned*
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.200 BTU-in/hr-ft²-°F12% Moisture Content
 1.00 BTU-in/hr-ft²-°FOven Dry
Shrinkage 4.9 %Radial; Green to Zero Moisture
 9.5 %Tangential; Green to Zero Moisture
 14.9 %Volumetric; Green to Zero Moisture
 
Descriptive Properties
ColorCreamy whiteUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Yellow Birch Wood
Paper Birch Wood
Sweet Birch Wood
Black Maple Wood
Bigleaf Maple Wood

PTSAU / 71304

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.