MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Saflex® SG41 Interlayer
Material Notes: Saflex® SG solar interlayer is a high visible light, solar absorbing technology designed to enhance solar heat gain performance as compared to monolithic clear glass and laminates made with standard clear polyvinyl butyral (PVB) interlayer. It has the capability to meet or exceed many regulations for laminated safety glazing when properly selected, laminated, and installed. Plus, Saflex SG is specifically formulated to provide exceptional durability when exposed to natural weathering. Saflex SG interlayer also provides all the benefits of safety glazing, glass shard containment, structural integrity, sound abatement, security and storm protection when used in the proper configurations.

Benefits:

  • 0.55 Solar Heat Gain Coefficient (SHGC)
  • Visible Light Transmittance > 70%.
  • Uniform appearance over both flat and curved façades
  • Edge deletion not required
  • Reduces angular color concerns
  • Reduces outside noise
Applications: Large glass facades - Curtain walls - Storefronts - Skylights - Windows

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 37 %Solar; ISO 9050
 76 %Light; ISO 9050
UV Transmittance <= 0.010 %ISO 9050
Reflection Coefficient, Visible (0-1) 0.050Solar, ISO 9050
 0.070Light, ISO 9050
 
Descriptive Properties
Damage Weighted Factor0.23ISO 9050
Light to Solar Gain1.4ISO 9050
Shading Coefficient0.64ISO 9050
Solar Heat Gain Coefficient0.55ISO 9050
U factor5.66 W/m2-KISO 9050

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Saflex® 0.060 inch Clear Protective Interlayer PVB Film for Glass Laminates
A. Schulman FORMION™ FI 392 Ionomer
Eastman XIR 70.48 Film
Evonik DYNACOLL® AC 1420 Polyacrylate
Eastman Saflex® RB11 Clear PVB interlayer

PEAT7017 / 183585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.