MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm PLEXIGLAS® Satinice df20 8N PMMA  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Product Profile: PLEXIGLAS® Satinice df20 8N based on PLEXIGLAS® 8N are characterized by diffuse scattering of light. Besides showing the familiar properties of standard PLEXIGLAS® molding compound, such as
  • excellent weatherability,
  • high surface hardness and mar resistance,
PLEXIGLAS® Satinice df20 8N is special in that they combine
  • good diffusing power with excellent light transmission.
Application: Used for injection molding items for lighting engineering applications

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Melt Flow 2.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 74.0 MPa5 mm/min; ISO 527
Elongation at Break 5.0 %5 mm/min; ISO 527
Tensile Modulus 3300 MPaISO 527
Charpy Impact Unnotched 19.0 kJ/m²ISO 179/1eU
 
Thermal PropertiesOriginal ValueComments
CTE, linear 63.0 µin/in-°F
@Temperature 0.000 - 50.0 °C
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 103 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °CISO 75
Vicat Softening Point 108 °CB/50; ISO 306
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 88 %ISO 13468-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 260 °C
Mold Temperature 60.0 - 90.0 °CInjection
Drying Temperature <= 95.0 °CPredrying
Dry Time 2.00 - 3.00 hourPredrying

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm Plexiglas® 8N PMMA Molding Compound
Röhm Plexiglas® df23 8N Molding Compound
Röhm Plexiglas® df21 8N Molding Compound
Röhm PLEXIGLAS® Satinice df23 7N PMMA
Röhm Plexiglas® df22 8N Molding Compound

PEVONIL160 / 196364

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.