MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lotte Advanced Materials Infino® AR-5300H PBT/ASA, 30% Glass Filled
Categories: Polymer; Thermoplastic; ASA Polymer; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + ASA Blend, Glass Fiber Reinforced

Material Notes:

Information provided by Samsung Cheil Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 3.20 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 30 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
Ash 30 %ASTM D5630
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 117ASTM D785
Tensile Strength at Break 127 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 1350 kg(f)/cm²5 mm/min; ASTM D638
Elongation at Break 5.0 %5 mm/min; ASTM D638
Tensile Modulus 90000 kg(f)/cm²5 mm/min; ASTM D638
Flexural Strength 186 MPa2.8 mm/min; ASTM D790
Flexural Modulus 95000 kg(f)/cm²2.8 mm/min; ASTM D790
Izod Impact, Notched 7.00 kg-cm/cm
@Thickness 6.35 mm
ASTM D256
 8.00 kg-cm/cm
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 205 °C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
@Thickness 6.40 mm
ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
Omni Plastics OmniTech™ PBSA GR30 PBT/ASA, 30% Glass Reinforced
Eurotec® Tecodur® PB70 GR30 NL MB04 PBT/ASA, 30% glass fiber reinforced, heat & UV stabilized, natural
Envalior Stanyl® TE351 PA46 FR(17), Dry, Flame Retardant, Heat Stabilized
Envalior Pocan® TP 740-202 901510 PBT+ASA, 20% Glass Fiber

PSAMSU703 / 146520

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.