MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultrason® E 2010 C6 30% Carbon Filled
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone, Carbon Fiber Reinforced

Material Notes: Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatures of up to 200 °C.

Excellent properties: very high stiffness, very constant mechanical properties, low and constant thermal expansion = dimensionally stable and excellent creep behavior

Potential applications: Substitution of metal, using the advantages of thermoplastic materials (e.g. realization of complex designs by injection-molding), substitution of PEEK for applications with a maximum of 200 °C, parts with antistatic requirements and parts with electrically conductive requirements

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.700 - 0.800 g/cc
Density 1.47 g/ccISO 1183
Water Absorption <= 1.7 %Equilibrium; ISO 62
Moisture Absorption at Equilibrium 0.60 %23°C; 50% RH; ISO 62
Viscosity Test 56 cm³/gISO 1628
Linear Mold Shrinkage, Flow 0.0015 cm/cmISO 294
Linear Mold Shrinkage, Transverse 0.0035 cm/cmISO 294
Melt Flow >= 22.05 g/10 min
@Load 10.0 kg,
Temperature 360 °C
ISO 1133
 >= 45 g/10 min
@Load 10.0 kg,
Temperature 400 °C
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 227 MPa
@Load 36.5 kg,
Time 30.0 sec
ISO 2039-1
Tensile Strength at Break 185 MPa5 mm/min; ISO 527-2
Tensile Strength, Yield 185 MPa50 mm/min; ISO 527-2
Elongation at Break 1.5 %5mm/min; ISO 527-2
Elongation at Yield 1.5 %50 mm/min; ISO 527-2
 0.21 %
@Time 3600 sec,
Pressure 50.0 MPa
ISO 899
 0.23 %
@Pressure 50.0 MPa,
Time 360000 sec
ISO 899
 0.24 %
@Pressure 50.0 MPa,
Time 3.60e+6 sec
ISO 899
 0.38 %
@Time 3600 sec,
Pressure 70.0 MPa
ISO 899
 0.40 %
@Pressure 70.0 MPa,
Time 360000 sec
ISO 899
 0.40 %
@Pressure 70.0 MPa,
Time 3.60e+6 sec
ISO 899
 0.50 %
@Time 3600 sec,
Pressure 90.0 MPa
ISO 899
 0.55 %
@Pressure 90.0 MPa,
Time 360000 sec
ISO 899
 0.58 %
@Pressure 90.0 MPa,
Time 3.60e+6 sec
ISO 899
 0.60 %
@Time 3600 sec,
Pressure 110 MPa
ISO 899
 0.70 %
@Time 360000 sec,
Pressure 110 MPa
ISO 899
 0.75 %
@Pressure 110 MPa,
Time 3.60e+6 sec
ISO 899
 0.80 %
@Time 3600 sec,
Pressure 130 MPa
ISO 899
 0.90 %
@Time 360000 sec,
Pressure 130 MPa
ISO 899
 0.98 %
@Pressure 130 MPa,
Time 3.60e+6 sec
ISO 899
Tensile Modulus >= 13000 MPa
@Temperature 200 °C
 >= 20000 MPa
@Temperature 150 °C
 >= 21000 MPa
@Temperature 100 °C
 >= 22000 MPa
@Temperature 50.0 °C
ISO 527-2
Shear Modulus 0.200 GPa
@Temperature 225 °C
ISO 6721
 0.900 GPa
@Temperature 200 °C
ISO 6721
 0.950 GPa
@Temperature 100 °C
ISO 6721
 1.00 GPa
@Temperature 50.0 °C
ISO 6721
Izod Impact, Notched (ISO) 8.00 kJ/m²ISO 180/A
 7.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
Charpy Impact Unnotched 40.0 kJ/m²ISO 179/1eU
 40.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 7.50 kJ/m²ISO 179/1eA
 6.50 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.9 ohm-cmIEC 60093
Surface Resistance >= 1000 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 4.00 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-1/-2
 4.00 µm/m-°C
@Temperature 140 - 180 °C
ISO 11359-1/-2
Maximum Service Temperature, Air 220 °Cshort cycle operations
Deflection Temperature at 1.8 MPa (264 psi) 225 °CISO 75-2
Glass Transition Temp, Tg 225 °CISO 11357-1/-2
Decomposition Temperature >= 400 °C
Flammability, UL94 V-0
@Thickness 1.60 mm
 V-0
@Thickness 3.20 mm
Ignition Temperature 580 - 600 °CDIN 54836
 
Processing PropertiesOriginal ValueComments
Melt Temperature 350 - 390 °CInjection molding/extrusion
 370 °COptimal
Mold Temperature 150 - 190 °CInjection molding
 170 °COptimal
Drying Temperature 140 °C
Dry Time 4 hour
 
Descriptive Properties
ColorBlack
Commercial StatusNorth America and Europe
Primary Processing TechniqueInjection Molding and Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 2299 X 115090 B Polyetheretherketone (PEEK), Carbon Nanotube - Electrically Conductive
RTP Company RTP 2287 HEC Polyetheretherketone (PEEK); Nickel-Coated Carbon Fiber - EMI/RFI Shielding - Electrically Conductive
RTP Company EMI 2263 Polyetheretherketone (PEEK), Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
RTP Company RTP 1499 P X 125056 A Polyphenyl Sulfone (PPSU) Stainless Steel Fiber - EMI/RFI Shielding
RTP Company RTP 2283 HEC Polyetheretherketone (PEEK), Nickel-Coated Carbon Fiber - EMI/RFI/ESD Protection - Electrically Conductive

PBASG0170 / 131803

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.