MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay ALKAMULS® T/20 Surfactant  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Polysorbate 20 Oil in water emulsifier for mineral and vegetable oils in metalworking. Solubilizer, antistat and lubricant fortextile industry. Nonionic sorbitan ester ethoxylate with an HLB of approx. 16.7. Useful as emulsifier for aliphatic oils and as a biological activator in adjuvants.

Identification: ETHOXYLATED SORBITAN MONOLAURATE

CAS: 9005 – 64 – 5

Solubility: Soluble in water and most polar and aromatic solvents.

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Agrochemical formulations: Useful as emulsifier for aliphatic oils and as a biologicalactivator in adjuvants. Industrial formulations: Oil in water emulsifier for mineral and vegetable oils in metalworking. Solubilizer, antistat and lubricant for textile industry. Metal treatment: Sorbitan ester ethoxylate with a HLB of 16.7. Oil in water emulsifier for mineral and vegetable oils in metalworking. Solubilizer, antistat and lubricant for textile industry. Polymer systems specialities : Ethoxylated emulsifier and dispersant.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
pH 6.0 - 8.06.0 - 8.05% in water; RPG02
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 2.0<= 2.0[mg KOH/g]; RPG03
 
Thermal PropertiesMetricEnglishComments
Pour Point <= 0.000 °C<= 32.0 °F
Flash Point >= 100 °C>= 212 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 3.0 %<= 3.0 %RPG16
 
Descriptive Properties
AppearanceLiquid
CompositionActive0.97
HLB number16.7
Hydroxyl Number95-115 mg KOH/gRPG06
Ionic ChargeNonionic
Saponification number40-50 mg KOH/gRPG05

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay ALKAMULS® S 20 Surfactant
Solvay ALKAMULS® S 80 Surfactant
Solvay RHODASURF® TDA-12 Surfactant
Teijin Panlite® L-1250J Polycarbonate, Hot Water Resistant Grade
Solvay ALKAMULS® OR 40 Surfactant

WRHOD060 / 137291

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.