MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Terraloy™ BP 10000A Thermoplastic Starch + LLDPE
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Notes: Terraloy™ BP-10001A is a Thermoplastic Starch/LLDPE ready-to-process compound that contains up to 30% of TPS renewable content. This compound is for blown film application.

Forms: Pellets

Additional Information: Biobased Content: < 30.0

Information Provided by Teknor Apex

Key Words: TPS, LLDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/ccASTM D792
Water Vapor Transmission 0.580 g/100 in²/day
Oxygen Transmission Rate 460 cc/100 in²/dayASTM D1922
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 480 %ASTM D882
Film Elongation at Break, TD 680 %ASTM D882
Secant Modulus 28.0 ksiMD; ASTM D882
 41.8 ksiTD; ASTM D882
Elmendorf Tear Strength MD 320 gASTM D1922
Elmendorf Tear Strength TD 620 gASTM D1922
Dart Drop Test 450 gASTM D1709
Film Tensile Strength at Break, MD 7690 psiASTM D882
Film Tensile Strength at Break, TD 4480 psiASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BiologiQ EcoStarch GS270 Thermoplastic Starch
Teknor Apex Terraloy™ BP 20001A Thermoplastic Starch + Copolyester
DuPont Biomax® TPS 2100
DuPont Biomax® TPS 2501
Teknor Apex Terraloy™ MB 10000A Thermoplastic Starch + LLDPE

PTEKNO806 / 128987

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.