MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dover Chemical BASE 107 Sulfurized Lard Oil Active Sulfurized Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Base 107 is a 17% sulfurized lard oil possessing outstanding solubility in refined petroleum oils and many synthetic base oils. Its lower viscosity facilitates ambient temperature blending. Base 107 is recommended for straight oil machining, drawing and stamping fluids, and can be formulated into soluble oils. Base 107 has 6% active sulfur, so it is not recommended for use in applications involving yellow metals (copper, brass and bronze). Base 107 may be stored in an original container or bulk storage tank. Prolonged exposure to 0°F may result in solidification. If the product solidifies, warming to 70-90°F will reconstitute the product. Recommended blending temperatures should not exceed 130°F.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc
@Temperature 25.0 °C
1.00 g/cc
@Temperature 77.0 °F
Density 0.995 g/cc0.0359 lb/in³
Saybolt Viscosity at 100°F 1600 SUS1600 SUS
Saybolt Viscosity at 210°F 160 SUS160 SUS
Kinematic Viscosity at 40°C (104°F) 265 cSt265 cSt
Kinematic Viscosity at 100°C (212°F) 30 cSt30 cSt
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 177 °C>= 351 °FCOC
 
Component Elements PropertiesMetricEnglishComments
Sulfur, S 6.0 %6.0 %Active
 17 %17 %Total
 
Descriptive Properties
Copper Corrosion410% in oil, 3 hrs, 210°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dover Chemical PRIME BURNING LARD OIL Lard Oil, Lubricity Additive
Dover Chemical MAYCO BASE 1210 Sulfurized Lard Oil, Non-Staining Sulfurized Additive
Dover Chemical EWS LARD OIL Lubricity Additive
Dover Chemical BASE 101 Sulfurized Lard Oil, Lubricity/Extreme Pressure Additive

WDOVER102 / 217721

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.