MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable
Categories: Ceramic; Machinable Ceramic; Nitride

Material Notes: Shapal-M® soft is a high purity, machinable ceramic with high strength and high thermal conductivity. Although the thermal conductivity is not as high as Aluminum Nitride, it is still 50 times that of machinable glass ceramic. Like aluminum nitride, applications include heat sinks and electronically insulating components for the high power electronic industry, and crucibles for molten metals. Shapal-M® also has the advantage that much more complex shapes may be used. It may be machined by using carbide tools and is resistant to acids and bases.

Information provided by Goodfellow. SHAPAL™-M is a trademark of Tokuyama Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.95 g/cc
Porosity 0.00 %Apparent Porosity
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 390
@Load 0.300 kg
kg/mm²
Tensile Modulus 186 GPa
Flexural Strength 294 MPa
Compressive Strength 1180 MPa
Poissons Ratio 0.31
Shear Modulus 71.0 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+12 ohm-cm
@Temperature 25.0 °C
Dielectric Constant 7.1
@Frequency 1e+6 Hz
Dielectric Strength 40.0 kV/mm
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.40 µm/m-°C
@Temperature 20.0 - 400 °C
 4.80 µm/m-°C
@Temperature 20.0 - 600 °C
 5.10 µm/m-°C
@Temperature 20.0 - 800 °C
Thermal Conductivity 80.0 W/m-K
@Temperature 200 °C
 86.0 W/m-K
@Temperature 100 °C
 90.0 W/m-K
@Temperature 25.0 °C
Maximum Service Temperature, Air 1000 °C
Maximum Service Temperature, Inert 1900 °C
 
Descriptive Properties
Acid Resistance0.2 mg/cm² wt. loss10% HCl (24 hrs.; 25°C)
Alkali Resistance60 mg/cm² wt. loss10% NaOH (24 hrs.; 25°C)
Thermal Shock Resistance (ΔT)400°CWater Quench

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum Nitride, AlN
Aremco AREMCOLOX™ 502-1800 Machinable Aluminum Nitride
MarkeTech AN 90 Aluminum Nitride Ceramic Substrate, 98% Purity
Tokuyama Shapal™ SH-15 Sintered Aluminum Nitride
MarkeTech AN 180 Aluminum Nitride Ceramic Substrate, 99% Purity

CGOODF107 / 939

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.