MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.

Uses: Blown and flat die/cast film extrusion, Injection molding and cable jacketing.

Information provided by Lubrizol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 82
@Time 5.00 sec
ASTM D2240
Tensile Strength 37.9 MPaASTM D412
 28.42 MPa
@Temperature 75.0 °C,
Time 4.838e+6 sec
Immersion in Water
 29.18 MPa
@Temperature 75.0 °C,
Time 2.59e+6 sec
Immersion in Water
 29.94 MPa
@Temperature 75.0 °C,
Time 1.21e+6 sec
Immersion in Water
 30.69 MPa
@Temperature 75.0 °C,
Time 605000 sec
Immersion in Water
 37.9 MPa
@Temperature 75.0 °C,
Time 0.000 sec
Immersion in Water
Elongation at Break 700 %ASTM D412
100% Modulus 0.00480 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.00760 GPa
@Strain 300 %
ASTM D412
Tear Strength 130 pliASTM D470
Graves Tear Strength 400 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 22H18, 1000g; ASTM D3389 B
Tensile Set 11 %200% elongation; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Melting Point 125 °CKofler
 130 °CDSC
Glass Transition Temp, Tg -50.0 °CDSC
 
Optical PropertiesOriginal ValueComments
Haze 7.0 %pressed between glass; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Zone 1 166 °CExtrusion
Zone 2 171 °CExtrusion
Zone 3 177 °CExtrusion
Zone 4 182 °CExtrusion
Adapter Temperature 182 °CExtrusion
Die Temperature 182 °CZone 1, Extrusion
 182 °CZone 2, Extrusion
Drying Temperature 104 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C
 
Descriptive Properties
Volume Swell in Water2%24h/23°C, ASTM D471

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58211 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane

PNOVEON046 / 55313

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.