MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Extir® CM Galileo Europa 5 Expandable Polystyrene - Continuous Mass
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Product Description:
  • Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of blowing agent. Extir CM does not contain CFC or HCFC. Extir CM Galileo Europa 5 contains an atherman additive that reduces heat transfer, and the items produced with it, gray in color, have excellent thermal insulation properties. Its unique formula allows the use of thinner boards to achieve the same thermal resistance.

    Applications: Extir CM Galileo Europa 5 reaches top performances as thermal insulation. It is highly recommended for all applications in which thickness is a limiting factor and fire resistance is not compulsory:

    • cavity wall insulation
    • thermoacoustic panels coupled with plasterboard.

    Information provided by Polimeri Europa.

    Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.590 - 0.630 g/cc0.0213 - 0.0228 lb/in³
Density >= 0.0120 g/cc>= 0.000434 lb/in³Minimum apparent density on a continuous pre-expander after two expansions
 >= 0.0160 g/cc>= 0.000578 lb/in³Minimum apparent density on a discontinuous pre-expander
 >= 0.0180 g/cc>= 0.000650 lb/in³Minimum apparent density on a continuous pre-expander after one expansion
 0.0120 - 0.0250 g/cc0.000434 - 0.000903 lb/in³Density range normally used
Particle Size 900 - 1600 µm900 - 1600 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
LG Chemical R160 EPS, Flame Retardant
Sekisui PIOCELAN SP-50D Moldable Polymer Foam
LG Chemical R320 EPS, Flame Retardant
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer

PENG160 / 124554

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.