MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Nylon 66, 30% Mineral Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Mineral Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.30 - 1.62 g/ccAverage value: 1.39 g/cc Grade Count:46
 1.40 - 1.40 g/cc
@Temperature 290 - 290 °C
Average value: 1.40 g/cc Grade Count:1
Filler Content 25.0 - 32.0 %Average value: 29.5 % Grade Count:6
Water Absorption 0.400 - 6.20 %Average value: 1.80 % Grade Count:22
Moisture Absorption at Equilibrium 0.170 - 2.30 %Average value: 1.49 % Grade Count:10
Water Absorption at Saturation 5.00 - 8.00 %Average value: 5.80 % Grade Count:5
Maximum Moisture Content 0.0900 - 0.150Average value: 0.110 Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.0200 cm/cmAverage value: 0.0100 cm/cm Grade Count:43
Linear Mold Shrinkage, Transverse 0.00600 - 0.0200 cm/cmAverage value: 0.0117 cm/cm Grade Count:18
Melt Flow 1.00 - 20.0 g/10 minAverage value: 7.33 g/10 min Grade Count:6
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90.0Average value: 90.0 Grade Count:3
Hardness, Rockwell R 115 - 125Average value: 120 Grade Count:14
Tensile Strength, Ultimate 40.0 - 159 MPaAverage value: 74.6 MPa Grade Count:34
Tensile Strength, Yield 73.5 - 186 MPaAverage value: 98.9 MPa Grade Count:13
Elongation at Break 1.00 - 50.0 %Average value: 8.66 % Grade Count:38
Elongation at Yield 3.00 - 16.0 %Average value: 8.33 % Grade Count:3
Modulus of Elasticity 1.90 - 9.31 GPaAverage value: 5.06 GPa Grade Count:22
Flexural Yield Strength 50.0 - 241 MPaAverage value: 128 MPa Grade Count:31
Flexural Modulus 1.80 - 9.65 GPaAverage value: 4.73 GPa Grade Count:38
Poissons Ratio 0.350 - 0.410Average value: 0.369 Grade Count:4
Izod Impact, Notched 0.196 - 1.10 J/cmAverage value: 0.531 J/cm Grade Count:22
Izod Impact, Unnotched 2.67 - 14.9 J/cmAverage value: 8.19 J/cm Grade Count:3
Izod Impact, Notched (ISO) 2.00 - 330 kJ/m²Average value: 36.0 kJ/m² Grade Count:12
 1.90 - 100 kJ/m²
@Temperature -40.0 - -30.0 °C
Average value: 23.7 kJ/m² Grade Count:5
Izod Impact, Unnotched (ISO) 9.00 - 330 kJ/m²Average value: 105 kJ/m² Grade Count:4
 5.00 - 85.0 kJ/m²
@Temperature -40.0 - -30.0 °C
Average value: 34.6 kJ/m² Grade Count:3
Charpy Impact Unnotched 1.80 J/cm² - NBAverage value: 8.38 J/cm² Grade Count:20
 1.10 - 12.0 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 4.57 J/cm² Grade Count:14
Charpy Impact, Notched 0.200 - 1.50 J/cm²Average value: 0.585 J/cm² Grade Count:18
 0.150 - 1.00 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 0.433 J/cm² Grade Count:12
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+11 - 1.00e+17 ohm-cmAverage value: 9.16e+15 ohm-cm Grade Count:21
Surface Resistance 1.00e+10 - 1.00e+15 ohmAverage value: 9.68e+13 ohm Grade Count:11
Dielectric Constant 3.40 - 9.10Average value: 4.40 Grade Count:9
Dielectric Strength 15.0 - 85.0 kV/mmAverage value: 34.2 kV/mm Grade Count:21
Dissipation Factor 0.0100 - 0.0500Average value: 0.0219 Grade Count:4
Comparative Tracking Index 300 - 600 VAverage value: 471 V Grade Count:13
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.8 - 65.0 µm/m-°CAverage value: 49.0 µm/m-°C Grade Count:14
CTE, linear, Transverse to Flow 65.0 - 81.0 µm/m-°CAverage value: 75.3 µm/m-°C Grade Count:3
Specific Heat Capacity 1.70 - 1.70 J/g-°C
@Temperature 290 - 290 °C
Average value: 1.70 J/g-°C Grade Count:1
Thermal Conductivity 0.230 - 0.230 W/m-K
@Temperature 290 - 290 °C
Average value: 0.230 W/m-K Grade Count:1
Melting Point 254 - 265 °CAverage value: 259 °C Grade Count:31
Maximum Service Temperature, Air 80.0 - 220 °CAverage value: 130 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 145 - 260 °CAverage value: 224 °C Grade Count:25
Deflection Temperature at 1.8 MPa (264 psi) 60.0 - 256 °CAverage value: 147 °C Grade Count:41
Vicat Softening Point 200 - 265 °CAverage value: 236 °C Grade Count:17
Flammability, UL94 HB - 5VAGrade Count:30
Flame Spread 0.000 - 80.0 mm/minAverage value: 53.3 mm/min Grade Count:3
Oxygen Index 24.0 - 40.0 %Average value: 28.6 % Grade Count:8
Glow Wire Test 649 - 960 °CAverage value: 772 °C Grade Count:14
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 250 - 295 °CAverage value: 279 °C Grade Count:4
Melt Temperature 250 - 310 °CAverage value: 283 °C Grade Count:27
Mold Temperature 50.0 - 120 °CAverage value: 90.1 °C Grade Count:26
Drying Temperature 79.4 - 100 °CAverage value: 85.2 °C Grade Count:22
Moisture Content 0.0300 - 0.200 %Average value: 0.167 % Grade Count:11
Injection Pressure 34.5 - 138 MPaAverage value: 95.2 MPa Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, 10% Mineral Filled
Overview of materials for Nylon 66, 20% Mineral Filled
Overview of materials for Nylon 66, 40% Mineral Filled
BASF Ultramid® A3HG5 25% Glass Filled PA66 (Dry)
BASF Ultramid® A3HG5 25% Glass Filled PA66 (Conditioned)

O2533 / 78030

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.